nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A growth rule for regular polygons with arcs as sides
|
Nordbakke, M.W. |
|
2007 |
56 |
1 |
p. 37-39 3 p. |
artikel |
2 |
A new algorithm to treat ternary diffusion couples with α/α+β boundaries
|
Liu, Yajun |
|
2007 |
56 |
1 |
p. 21-24 4 p. |
artikel |
3 |
Cation ordering in the microwave dielectric ceramic BaCd1/3Nb2/3O3
|
Deng, Jinxia |
|
2007 |
56 |
1 |
p. 65-68 4 p. |
artikel |
4 |
Effect of film thickness and annealing temperature on hillock distributions in pure Al films
|
Hwang, Soo-Jung |
|
2007 |
56 |
1 |
p. 17-20 4 p. |
artikel |
5 |
Effect of shrinkage flow on particle engulfment
|
Hadji, Layachi |
|
2007 |
56 |
1 |
p. 57-60 4 p. |
artikel |
6 |
Effect of sintering temperature on grain boundary character distribution in pure nickel
|
Bhattacharjee, P.P. |
|
2007 |
56 |
1 |
p. 13-16 4 p. |
artikel |
7 |
Effect of welding parameters on tensile properties and fracture behavior of friction stir welded Al–Mg–Si alloy
|
Ren, S.R. |
|
2007 |
56 |
1 |
p. 69-72 4 p. |
artikel |
8 |
Effect of ZrF4 on hot-pressed hydroxyapatite/monoclinic zirconia composites
|
Evis, Zafer |
|
2007 |
56 |
1 |
p. 53-56 4 p. |
artikel |
9 |
Electron microscopy study of nanocrystalline copper deformed by a microhardness indenter
|
Gai, Pratibha L. |
|
2007 |
56 |
1 |
p. 25-28 4 p. |
artikel |
10 |
First-principles study of the effect of hydrogen on the Ti self-diffusion characteristics in the alpha Ti–H system
|
Han, X.L. |
|
2007 |
56 |
1 |
p. 77-80 4 p. |
artikel |
11 |
Microwave sintering of W–Ni–Fe alloy
|
Upadhyaya, A. |
|
2007 |
56 |
1 |
p. 5-8 4 p. |
artikel |
12 |
Preparation of homogeneous Pb(Zr x Ti1−x )O3 by a rapid-quenching technique and its compositional fluctuation
|
Han, Young-Hwan |
|
2007 |
56 |
1 |
p. 9-12 4 p. |
artikel |
13 |
Processing of copper fiber-reinforced Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 bulk metallic glass composites
|
Wadhwa, Prashant |
|
2007 |
56 |
1 |
p. 73-76 4 p. |
artikel |
14 |
Rapid growth of tin whiskers on the surface of Sn–6.6Lu alloy
|
Chuang, T.H. |
|
2007 |
56 |
1 |
p. 45-48 4 p. |
artikel |
15 |
Solidification path in third-generation Ni-based superalloys, with an emphasis on last stage solidification
|
D’Souza, N. |
|
2007 |
56 |
1 |
p. 41-44 4 p. |
artikel |
16 |
Suppressing Ni–Sn–P growth in SnAgCu/Ni–P solder joints
|
Lin, Yung-Chi |
|
2007 |
56 |
1 |
p. 49-52 4 p. |
artikel |
17 |
The crack initiation mechanism of the forged Mg–Zn–Y–Zr alloy in the super-long fatigue life regime
|
Xu, D.K. |
|
2007 |
56 |
1 |
p. 1-4 4 p. |
artikel |
18 |
The formation of ordered structures in InGaN layers
|
Rao, M. |
|
2007 |
56 |
1 |
p. 33-36 4 p. |
artikel |
19 |
The recovery of structural relaxation-induced viscoelastic creep strain in bulk and ribbon Pd40Cu30Ni10P20 glass
|
Bobrov, O.P. |
|
2007 |
56 |
1 |
p. 29-32 4 p. |
artikel |
20 |
Trans-interface diffusivity in the Fe–Ni system
|
Larsson, Henrik |
|
2007 |
56 |
1 |
p. 61-64 4 p. |
artikel |