nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
An alternative magnesium-based root canal disinfectant: Preliminary study of its efficacy against Enterococcus faecalis and Candida albicans in vitro
|
Zhu, Lin |
|
2014 |
24 |
5 |
p. 441-445 5 p. |
artikel |
2 |
Biodegradable intestinal stents: A review
|
Wang, Zhanhui |
|
2014 |
24 |
5 |
p. 423-432 10 p. |
artikel |
3 |
Corrosion mechanism of micro-arc oxidation treated biocompatible AZ31 magnesium alloy in simulated body fluid
|
Li, Ying |
|
2014 |
24 |
5 |
p. 516-522 7 p. |
artikel |
4 |
Corrosion of magnesium and magnesium–calcium alloy in biologically-simulated environment
|
Harrison, Richard |
|
2014 |
24 |
5 |
p. 539-546 8 p. |
artikel |
5 |
Doping inorganic ions to regulate bioactivity of Ca–P coating on bioabsorbable high purity magnesium
|
Wu, Hongliu |
|
2014 |
24 |
5 |
p. 479-485 7 p. |
artikel |
6 |
Effects of solidification cooling rate on the corrosion resistance of Mg–Zn–Ca alloy
|
Liu, Debao |
|
2014 |
24 |
5 |
p. 452-457 6 p. |
artikel |
7 |
Engineered polycaprolactone–magnesium hybrid biodegradable porous scaffold for bone tissue engineering
|
Wong, Hoi Man |
|
2014 |
24 |
5 |
p. 561-567 7 p. |
artikel |
8 |
Facile immobilization of heparin on bioabsorbable iron via mussel adhesive protein (MAPs)
|
Xu, Xuchen |
|
2014 |
24 |
5 |
p. 458-465 8 p. |
artikel |
9 |
Forming of magnesium alloy microtubes in the fabrication of biodegradable stents
|
Wang, Lixiao |
|
2014 |
24 |
5 |
p. 500-506 7 p. |
artikel |
10 |
Impact behaviors of poly-lactic acid based biocomposite reinforced with unidirectional high-strength magnesium alloy wires
|
Li, Xuan |
|
2014 |
24 |
5 |
p. 472-478 7 p. |
artikel |
11 |
Influence of HEPES buffer on the local pH and formation of surface layer during in vitro degradation tests of magnesium in DMEM
|
Naddaf Dezfuli, S. |
|
2014 |
24 |
5 |
p. 531-538 8 p. |
artikel |
12 |
Influence of the extraction parameters on the cytotoxicity test results of Mg materials
|
Liu, Xiaoli |
|
2014 |
24 |
5 |
p. 507-515 9 p. |
artikel |
13 |
Investigation on magnesium degradation under flow versus static conditions using a novel impedance-driven flow apparatus
|
Mai, Elbert David |
|
2014 |
24 |
5 |
p. 554-560 7 p. |
artikel |
14 |
In vitro and in vivo studies on biodegradable magnesium alloy
|
Hou, Lida |
|
2014 |
24 |
5 |
p. 466-471 6 p. |
artikel |
15 |
In vitro corrosion of Mg–1.21Li–1.12Ca–1Y alloy
|
Zeng, Rongchang |
|
2014 |
24 |
5 |
p. 492-499 8 p. |
artikel |
16 |
Optimization of dual effects of Mg–1Ca alloys on the behavior of chondrocytes and osteoblasts in vitro
|
Dou, Yana |
|
2014 |
24 |
5 |
p. 433-440 8 p. |
artikel |
17 |
Preface
|
|
|
2014 |
24 |
5 |
p. 413- 1 p. |
artikel |
18 |
Preparation, microstructure and degradation performance of biomedical magnesium alloy fine wires
|
Bai, Jing |
|
2014 |
24 |
5 |
p. 523-530 8 p. |
artikel |
19 |
Progress of biodegradable metals
|
Li, Huafang |
|
2014 |
24 |
5 |
p. 414-422 9 p. |
artikel |
20 |
Study on vertical mandibular distraction osteogenesis using magnesium alloy on canine
|
Wang, Chengyue |
|
2014 |
24 |
5 |
p. 446-451 6 p. |
artikel |
21 |
Surface characteristics and corrosion resistance of biodegradable magnesium alloy ZK60 modified by Fe ion implantation and deposition
|
Zheng, Yang |
|
2014 |
24 |
5 |
p. 547-553 7 p. |
artikel |
22 |
The enhanced corrosion resistance of UMAO coatings on Mg by silane treatment
|
Li, Muqin |
|
2014 |
24 |
5 |
p. 486-491 6 p. |
artikel |