nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Coercive force and strength of carbon steel
|
Sandomirskii, S. G. |
|
2016 |
46 |
9 |
p. 671-674 |
artikel |
2 |
Continuous reductive smelting of steel
|
Tleugabulov, S. M. |
|
2016 |
46 |
9 |
p. 651-656 |
artikel |
3 |
Converter smelting of steel with preliminary scrap heating to reduce hot-metal consumption
|
Pak, Yu. A. |
|
2016 |
46 |
9 |
p. 657-661 |
artikel |
4 |
Corrosion resistance of high-strength austenitic chromium–nickel–manganese steel containing nitrogen
|
Kaputkina, L. M. |
|
2016 |
46 |
9 |
p. 644-650 |
artikel |
5 |
Decarburization of high-chromium melts by argon–oxygen plasma
|
Rumyantsev, B. A. |
|
2016 |
46 |
9 |
p. 638-643 |
artikel |
6 |
Design of new precision alloys
|
Molotilov, B. V. |
|
2016 |
46 |
9 |
p. 675-678 |
artikel |
7 |
Dynamic model of the ladle treatment of steel
|
Tikhonov, G. I. |
|
2016 |
46 |
9 |
p. 662-664 |
artikel |
8 |
Extraction of iron from copper-plant slag
|
Lykasov, A. A. |
|
2016 |
46 |
9 |
p. 609-613 |
artikel |
9 |
Formation of metallic phase by passing gaseous reducing agent through multicomponent oxide melt. Part 1. Theoretical principles
|
Vusikhis, A. S. |
|
2016 |
46 |
9 |
p. 629-632 |
artikel |
10 |
Influence of the packing-defect energy on the abrasive wear resistance of Fe–12Mn–1.2C steel castings cooled at different rates
|
Vdovin, K. N. |
|
2016 |
46 |
9 |
p. 614-619 |
artikel |
11 |
Influence of the temperature and strain rate on the deformability of low-alloy carbon steel
|
Laber, K. B. |
|
2016 |
46 |
9 |
p. 620-623 |
artikel |
12 |
Predicting the liquidus temperature of complex nickel alloys
|
Zubarev, K. A. |
|
2016 |
46 |
9 |
p. 633-637 |
artikel |
13 |
Surface-crack formation in the manufacture of microalloyed steel pipe
|
Kolbasnikov, N. G. |
|
2016 |
46 |
9 |
p. 665-670 |
artikel |
14 |
Thermal state of air tuyeres in blast furnaces
|
Radyuk, A. G. |
|
2016 |
46 |
9 |
p. 624-628 |
artikel |