nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Э90AΦ steel rail
|
Yur’ev, A. B. |
|
2008 |
38 |
7 |
p. 589-591 |
artikel |
2 |
Development of continuous casting at OAO MMK
|
Takhautdinov, R. S. |
|
2008 |
38 |
7 |
p. 556-559 |
artikel |
3 |
Improving the production of granulated FS15G ferrosilicon
|
Tutubalin, S. V. |
|
2008 |
38 |
7 |
p. 569-570 |
artikel |
4 |
Improving the shape and flatness of hot-rolled strip by means of profil 2500 software
|
Salganik, V. M. |
|
2008 |
38 |
7 |
p. 571-573 |
artikel |
5 |
Influence of incomplete weakening of metal on the yield point in continuous hot rolling of broad steel strip
|
Nikolaev, V. A. |
|
2008 |
38 |
7 |
p. 525-527 |
artikel |
6 |
Influence of low-frequency treatment on the mechanical properties and internal stress of weld-seam metal in structural steel
|
Tsvetkov, A. S. |
|
2008 |
38 |
7 |
p. 531-532 |
artikel |
7 |
Innovative linings for continuous-furnace hearths
|
Krasnyi, B. L. |
|
2008 |
38 |
7 |
p. 577-579 |
artikel |
8 |
Kinetics of the carbon reduction of liquid copper
|
Ten, E. B. |
|
2008 |
38 |
7 |
p. 533-536 |
artikel |
9 |
Manufacturing injection units for intermediate ladles at OAO MMK
|
Bosyakova, N. A. |
|
2008 |
38 |
7 |
p. 562-564 |
artikel |
10 |
Metallurgy of bearing steel
|
Molotilov, B. V. |
|
2008 |
38 |
7 |
p. 565-568 |
artikel |
11 |
Modernizing curvilinear continuous-casting machines with a vertical section
|
Sarychev, A. V. |
|
2008 |
38 |
7 |
p. 560-561 |
artikel |
12 |
Pellet heating and melting in the combustion zone of an electric arc
|
Kozhukhov, A. A. |
|
2008 |
38 |
7 |
p. 514-516 |
artikel |
13 |
Pipe rolling in helical-rolling mills without a guide system
|
Merkulov, D. V. |
|
2008 |
38 |
7 |
p. 580-584 |
artikel |
14 |
Producing high-basicity sinter from low-silica ore
|
Didevich, A. V. |
|
2008 |
38 |
7 |
p. 546-549 |
artikel |
15 |
Production of high-strength steel sheet for the auto industry
|
Kunitsyn, G. A. |
|
2008 |
38 |
7 |
p. 585-588 |
artikel |
16 |
Production of rolls of low-alloy rolled steel sheet for electrowelded pipe
|
Denisov, S. V. |
|
2008 |
38 |
7 |
p. 574-576 |
artikel |
17 |
Rational reduction of hot-rolled 40X steel before cold upsetting
|
Pachurin, G. V. |
|
2008 |
38 |
7 |
p. 522-524 |
artikel |
18 |
Seventy-five years of rolled-steel production in Magnitogorsk
|
Rashnikov, V. F. |
|
2008 |
38 |
7 |
p. 542-545 |
artikel |
19 |
Seventy-five years of steel production in Magnitogorsk
|
Rashnikov, V. F. |
|
2008 |
38 |
7 |
p. 537-541 |
artikel |
20 |
Size distribution of titanium-carbide grains in the liquid-phase sintering of Ni-TiC composite
|
Gurevich, Yu. G. |
|
2008 |
38 |
7 |
p. 528-530 |
artikel |
21 |
Slag segregation in steel discharge from an oxygen converter
|
Eron’ko, S. P. |
|
2008 |
38 |
7 |
p. 509-513 |
artikel |
22 |
Stability of strip rolling in vertical rollers
|
Aldunin, A. V. |
|
2008 |
38 |
7 |
p. 517-521 |
artikel |
23 |
Systems for reducing Kachkanarsk pellets
|
Rybkin, V. S. |
|
2008 |
38 |
7 |
p. 550-555 |
artikel |
24 |
Thermal stability of phases in iron-chromium-nitrogen alloys
|
Leonovich, B. I. |
|
2008 |
38 |
7 |
p. 505-508 |
artikel |