nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Al-to-Cu Friction Stir Lap Welding
|
Firouzdor, Vahid |
|
2011 |
43 |
1 |
p. 303-315 |
artikel |
2 |
A New Oxide Morphology Map: Initial Oxidation Behavior of Ni-Base Single-Crystal Superalloys
|
Suzuki, Aya S. |
|
2011 |
43 |
1 |
p. 155-162 |
artikel |
3 |
Comparison of High-Temperature Properties and Thermal Shock Resistance of Austempered Ductile Irons (ADI) with Those of Pearlitic Ductile Cast Irons
|
Ajabshiri, Mehrdad |
|
2011 |
43 |
1 |
p. 56-60 |
artikel |
4 |
Deformation-Induced Grain Refinement and Amorphization in Ti-10V-2Fe-3Al Alloy
|
Chen, Wei |
|
2011 |
43 |
1 |
p. 316-326 |
artikel |
5 |
Discontinuous Precipitation and Phase Stability In Re- and Ru-Containing Nickel-Base Superalloys
|
Heckl, Astrid |
|
2011 |
43 |
1 |
p. 10-19 |
artikel |
6 |
Effect of Sn on the Dehydrogenation Process of TiH2 in Al Foams
|
Aguirre-Perales, Lydia Y. |
|
2011 |
43 |
1 |
p. 1-5 |
artikel |
7 |
Effects of Alloying Elements on High-Temperature Oxidation and Sticking Occurring During Hot Rolling of Modified Ferritic STS430J1L Stainless Steels
|
Ha, Dae Jin |
|
2011 |
43 |
1 |
p. 74-86 |
artikel |
8 |
Effects of Processing Residual Stresses on Fatigue Crack Growth Behavior of Structural Materials: Experimental Approaches and Microstructural Mechanisms
|
Lammi, Christopher J. |
|
2011 |
43 |
1 |
p. 87-107 |
artikel |
9 |
Experimental and Modeling Studies of the Lamellar Eutectic Growth of Mg-Al Alloy
|
Xiong, Shou-mei |
|
2011 |
43 |
1 |
p. 208-218 |
artikel |
10 |
Finite-Element Modeling of Titanium Powder Densification
|
Ye, Bing |
|
2011 |
43 |
1 |
p. 381-390 |
artikel |
11 |
Fluid Flow and Defect Formation in the Three-Dimensional Dendritic Structure of Nickel-Based Single Crystals
|
Madison, J. |
|
2011 |
43 |
1 |
p. 369-380 |
artikel |
12 |
Improvement in Fatigue Strength of Biomedical β-type Ti–Nb–Ta–Zr Alloy While Maintaining Low Young’s Modulus Through Optimizing ω-Phase Precipitation
|
Nakai, Masaaki |
|
2011 |
43 |
1 |
p. 294-302 |
artikel |
13 |
Influence of Aging and Thermomechanical Treatments on the Mechanical Properties of a Nanocluster-Strengthened Ferritic Steel
|
Zhang, Z. W. |
|
2011 |
43 |
1 |
p. 351-359 |
artikel |
14 |
Influence of Aging Parameters on the Tensile Properties and Quality Index of Al-9 Pct Si-1.8 Pct Cu-0.5 Pct Mg 354-Type Casting Alloys
|
Ammar, H. R. |
|
2011 |
43 |
1 |
p. 61-73 |
artikel |
15 |
Influence of Aluminum on the Formation Behavior of Zn-Al-Fe Intermetallic Particles in a Zinc Bath
|
Park, Joo Hyun |
|
2011 |
43 |
1 |
p. 195-207 |
artikel |
16 |
Influence of Thermal Aging on the Microstructure and Mechanical Behavior of Dual-Phase, Precipitation-Hardened, Powder Metallurgy Stainless Steels
|
Stewart, J. L. |
|
2011 |
43 |
1 |
p. 124-135 |
artikel |
17 |
Interfacial Microstructure in a B4C/Al Composite Fabricated by Pressureless Infiltration
|
Luo, Zhiping |
|
2011 |
43 |
1 |
p. 281-293 |
artikel |
18 |
Laser Keyhole Welding of Dissimilar Ti-6Al-4V Titanium Alloy to AZ31B Magnesium Alloy
|
Gao, M. |
|
2011 |
43 |
1 |
p. 163-172 |
artikel |
19 |
Martensitic Transformation During Cold Rolling Deformation of an Austenitic Fe-26Mn-0.14C Alloy
|
Sahu, P. |
|
2011 |
43 |
1 |
p. 47-55 |
artikel |
20 |
Modeling and Prediction of Hot Deformation Flow Curves
|
Mirzadeh, Hamed |
|
2011 |
43 |
1 |
p. 108-123 |
artikel |
21 |
On the Effect of Manganese on Grain Size Stability and Hardenability in Ultrafine-Grained Ferrite/Martensite Dual-Phase Steels
|
Calcagnotto, Marion |
|
2011 |
43 |
1 |
p. 37-46 |
artikel |
22 |
On the Processing of Martensitic Steels in Continuous Galvanizing Lines: Part 1
|
Song, Taejin |
|
2011 |
43 |
1 |
p. 245-262 |
artikel |
23 |
On the Processing of Martensitic Steels in Continuous Galvanizing Lines: Part II
|
Song, Taejin |
|
2011 |
43 |
1 |
p. 263-280 |
artikel |
24 |
On the Role of Grain Boundary Serration in Simulated Weld Heat-Affected Zone Liquation of a Wrought Nickel-Based Superalloy
|
Hong, Hyun Uk |
|
2011 |
43 |
1 |
p. 173-181 |
artikel |
25 |
Oxidation Behavior of Nb-20Mo-15Si-25Cr and Nb-20Mo-15Si-25Cr-5B Alloys
|
Portillio, Benedict I. |
|
2011 |
43 |
1 |
p. 147-154 |
artikel |
26 |
Phase Diagrams of the Zr–Si–RE (RE=La and Er) Ternary Systems at 773 K (500 °C)
|
Li, Chunliu |
|
2011 |
43 |
1 |
p. 20-28 |
artikel |
27 |
Phase Equilibria of the Al–V–RE (RE = Gd, Ho) Systems at 773 K (500 °C)
|
Zhan, Yongzhong |
|
2011 |
43 |
1 |
p. 29-36 |
artikel |
28 |
Protection by Thermal and Chemical Activation with Cerium Salts of the Alloy AA2017 in Aqueous Solutions of NaCl
|
Bethencourt, Manuel |
|
2011 |
43 |
1 |
p. 182-194 |
artikel |
29 |
Ridging Control in Transformable Ferritic Stainless Steels
|
Mola, Javad |
|
2011 |
43 |
1 |
p. 228-244 |
artikel |
30 |
Role of Localized Deformation in Irradiation-Assisted Stress Corrosion Cracking Initiation
|
West, Elaine A. |
|
2011 |
43 |
1 |
p. 136-146 |
artikel |
31 |
Solidification Microstructure and Mechanical Properties of Cast Magnesium-Aluminum-Tin Alloys
|
Luo, Alan A. |
|
2011 |
43 |
1 |
p. 360-368 |
artikel |
32 |
Spark Plasma Sintering of Cryomilled Nanocrystalline Al Alloy - Part II: Influence of Processing Conditions on Densification and Properties
|
Liu, Dongming |
|
2011 |
43 |
1 |
p. 340-350 |
artikel |
33 |
Spark Plasma Sintering of Cryomilled Nanocrystalline Al Alloy - Part I: Microstructure Evolution
|
Xiong, Yuhong |
|
2011 |
43 |
1 |
p. 327-339 |
artikel |
34 |
Synthesis of In2O3 Thin Films from Indium Thin Film by Hot-Water Oxidation Method
|
Shanmugan, Subramani |
|
2011 |
43 |
1 |
p. 6-9 |
artikel |
35 |
Thermal-Treated Pitches as Binders for TiB2/C Composite Cathodes
|
Lü, Xiao-Jun |
|
2011 |
43 |
1 |
p. 219-227 |
artikel |