nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A Commentary on: “Diffusion of Carbon in Austenite with a Discontinuity in Composition”
|
Bhadeshia, H.K.D.H. |
|
2010 |
41 |
7 |
p. 1605-1615 |
artikel |
2 |
Amorphous Zr-Based Foams with Aligned, Elongated Pores
|
Cox, Marie E. |
|
2009 |
41 |
7 |
p. 1706-1713 |
artikel |
3 |
Biocompatibility Study of Zirconium-Based Bulk Metallic Glasses for Orthopedic Applications
|
He, Wei |
|
2010 |
41 |
7 |
p. 1726-1734 |
artikel |
4 |
Bulk Metallic Glasses VI
|
|
|
2010 |
41 |
7 |
p. 1627 |
artikel |
5 |
Comparison of Fatigue Strengths of Bulk Metallic Glasses Produced by Tilt Casting and High-Pressure Casting
|
Yokoyama, Yoshihiko |
|
2010 |
41 |
7 |
p. 1780-1786 |
artikel |
6 |
Cooling Slope Casting Process for Synthesis of Bulk Metallic Glass Based Composites with Semisolid Structure
|
Makaya, Advenit |
|
2010 |
41 |
7 |
p. 1646-1657 |
artikel |
7 |
Corrosion and Microstructure Correlation in Molten LiCl-KCl Medium
|
Ravi Shankar, A. |
|
2010 |
41 |
7 |
p. 1815-1825 |
artikel |
8 |
Effect of Austempering Conditions on the Microstructure and Tensile Properties of Low Alloyed Sintered Steel
|
Campos, M. |
|
2010 |
41 |
7 |
p. 1847-1854 |
artikel |
9 |
Effect of Nb Concentration on Thermal Stability and Glass-Forming Ability of Soft Magnetic (Fe,Co)-Gd-Nb-B Glassy Alloys
|
Zhang, Wei |
|
2009 |
41 |
7 |
p. 1685-1690 |
artikel |
10 |
Effects of Reinforcements on Creep Resistance of Hybrid-Reinforced Titanium Matrix Composites
|
Xiao, Lv |
|
2010 |
41 |
7 |
p. 1855-1863 |
artikel |
11 |
Erratum to: The Effects of Composition and Microstructure on the Thermal Conductivity of Liquid-Phase-Sintered W-Cu
|
Johnson, John L. |
|
2010 |
41 |
7 |
p. 1871 |
artikel |
12 |
Evolution of Constitution, Structure, and Morphology in FeCo-Based Multicomponent Alloys
|
Li, R. |
|
2009 |
41 |
7 |
p. 1640-1645 |
artikel |
13 |
Fatigue and Fracture Behavior of a Ca-Based Bulk-Metallic Glass
|
Raphael, J. |
|
2009 |
41 |
7 |
p. 1775-1779 |
artikel |
14 |
Fatigue Softening of (Zr58Ni13.6Cu18Al10.4)99Nb1 Bulk Metallic Glass
|
Qiao, Dongchun |
|
2010 |
41 |
7 |
p. 1787-1791 |
artikel |
15 |
Feeding Mechanisms in High-Pressure Die Castings
|
Otarawanna, S. |
|
2010 |
41 |
7 |
p. 1836-1846 |
artikel |
16 |
Formation, Structure, and Crystallization Behavior of Cu-Based Bulk Glass-Forming Alloys
|
Louzguine-Luzgin, D.V. |
|
2009 |
41 |
7 |
p. 1664-1669 |
artikel |
17 |
Fracture Behavior in Cu46.5Zr46.5Al7 and Cu46.5Zr41.5Al7Y5 Bulk Metallic Glasses
|
Matteis, P. |
|
2010 |
41 |
7 |
p. 1767-1774 |
artikel |
18 |
Glass-Forming Ability and Competitive Crystalline Phases for Lightweight Ti-Be–Based Alloys
|
Zhang, Y. |
|
2010 |
41 |
7 |
p. 1670-1676 |
artikel |
19 |
Grain Refining of 409L Ferritic Stainless Steel Using Fe-Ti-N Master Alloy
|
Wang, Chao |
|
2010 |
41 |
7 |
p. 1616-1620 |
artikel |
20 |
Influence of the Substrate on the Creep of SN Solder Joints
|
Lee, K.-O. |
|
2010 |
41 |
7 |
p. 1805-1814 |
artikel |
21 |
Mapping Residual Stress Distributions at the Micron Scale in Amorphous Materials
|
Winiarski, Bartlomiej |
|
2009 |
41 |
7 |
p. 1743-1751 |
artikel |
22 |
Microstructural Analysis of a Laser-Processed Zr-Based Bulk Metallic Glass
|
Sun, H. |
|
2010 |
41 |
7 |
p. 1752-1757 |
artikel |
23 |
Microstructural Aspects of Grain Boundary Bulge in a Dynamically Recrystallized Mg-Al-Zn Alloy
|
Sun, D.K. |
|
2010 |
41 |
7 |
p. 1864-1870 |
artikel |
24 |
Ni-Nb-Sn Bulk Metallic Glass Matrix Composites Fabricated by Microwave-Induced Sintering Process
|
Xie, Guoqiang |
|
2009 |
41 |
7 |
p. 1714-1719 |
artikel |
25 |
Oxidation Behavior of a Pd43Cu27Ni10P20 Bulk Metallic Glass and Foam in Dry Air
|
Kai, W. |
|
2010 |
41 |
7 |
p. 1720-1725 |
artikel |
26 |
Prediction of Glass-Forming Compositions in Metallic Systems: Copper-Based Bulk Metallic Glasses in the Cu-Mg-Ca System
|
Laws, Kevin J. |
|
2010 |
41 |
7 |
p. 1699-1705 |
artikel |
27 |
Relaxation Behavior of Ca-Based Bulk Metallic Glasses
|
Senkov, Oleg N. |
|
2009 |
41 |
7 |
p. 1677-1684 |
artikel |
28 |
Roles of In-Situ Forming Hard Particles in a Zr-Based Bulk-Metallic Glass during Monotonic and Cyclic Loading
|
Wang, G.Y. |
|
2010 |
41 |
7 |
p. 1799-1804 |
artikel |
29 |
Solid-Liquid Interface Energy between Silicon Crystal and Silicon-Aluminum Melt
|
Jian, Zengyun |
|
2010 |
41 |
7 |
p. 1826-1835 |
artikel |
30 |
Specimen Size Effects on Zr-Based Bulk Metallic Glasses Investigated by Uniaxial Compression and Spherical Nanoindentation
|
Bei, H. |
|
2009 |
41 |
7 |
p. 1735-1742 |
artikel |
31 |
Statistical Mechanics of Metallic Glasses and Liquids
|
Egami, T. |
|
2010 |
41 |
7 |
p. 1628-1633 |
artikel |
32 |
Stress Corrosion and Corrosion Fatigue Crack Growth of Zr-Based Bulk Metallic Glass in Aqueous Solutions
|
Nakai, Y. |
|
2009 |
41 |
7 |
p. 1792-1798 |
artikel |
33 |
Stress-State Effects on the Fracture of a Zr-Ti-Ni-Cu-Be Bulk Amorphous Alloy
|
Varadarajan, R. |
|
2010 |
41 |
7 |
p. 1758-1766 |
artikel |
34 |
Structures at Glassy, Supercooled Liquid, and Liquid States in La-Based Bulk Metallic Glasses
|
Jiang, Q.K. |
|
2009 |
41 |
7 |
p. 1634-1639 |
artikel |
35 |
Thermomechanical Behavior of Cu50Hf41.5Al8.5 Bulk Metallic Glass after Sustained Elastic Deformation
|
Mubarok, A. |
|
2009 |
41 |
7 |
p. 1658-1663 |
artikel |
36 |
The Three-Dimensional Structure of Mg-Rich Plates in As-Cast Mg-Based Bulk Metallic Glass Composites
|
Robin, L. |
|
2009 |
41 |
7 |
p. 1691-1698 |
artikel |
37 |
Wetting of Polycrystalline α-Al2O3 by Molten Mg in Ar Atmosphere
|
Shen, Ping |
|
2010 |
41 |
7 |
p. 1621-1626 |
artikel |