nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
An experimental investigation of fretting fatigue in Ti-6Al-4V: the role of contact conditions and microstructure
|
Venkatesh, T. A. |
|
|
32 |
5 |
p. 1131-1146 |
artikel |
2 |
A process model for friction stir welding of age hardening aluminum alloys
|
Frigaard, Ø. |
|
|
32 |
5 |
p. 1189-1200 |
artikel |
3 |
Correlation of microstructure and surface roughness of disc drums fabricated by hot forging of an AISI 430F stainless steel
|
Kim, Dong-Kuk |
|
|
32 |
5 |
p. 1111-1118 |
artikel |
4 |
Creep-rupture behavior of a directionally solidified nickel-base superalloy
|
Guo, J. T. |
|
|
32 |
5 |
p. 1103-1110 |
artikel |
5 |
Dependency of fracture toughness on the inhomogeneity of coarse TiN particle distribution in a low alloy steel
|
Zhang, L. P. |
|
|
32 |
5 |
p. 1147-1155 |
artikel |
6 |
Dimensional anisotropy in 18 pct Ni maraging steel
|
Farooque, M. |
|
|
32 |
5 |
p. 1057-1061 |
artikel |
7 |
Discontinuous precipitation at [001] twist boundaries in Cu-0.75 wt pct Be alloy bicrystals
|
Monzen, R. |
|
|
32 |
5 |
p. 1075-1079 |
artikel |
8 |
Effect of growth velocity on the growth temperature of the Al-AlxFe eutectic in Al-2.85Fe-0.12V alloy
|
Wang, Y. |
|
|
32 |
5 |
p. 1251-1253 |
artikel |
9 |
Fracture toughness of alloy 600 and an EN82H weld in air and water
|
Mills, W. J. |
|
|
32 |
5 |
p. 1161-1174 |
artikel |
10 |
Hardness-depth profiling on nanometer scale
|
Kunert, M. |
|
|
32 |
5 |
p. 1201-1209 |
artikel |
11 |
Inclusions in commercial low and medium carbon ferromanganese
|
Sjöqvist, Thobias |
|
|
32 |
5 |
p. 1049-1056 |
artikel |
12 |
Influence of zirconium and copper on the early stages of aging in Al-Zn-Mg alloys
|
Jiang, X. J. |
|
|
32 |
5 |
p. 1063-1073 |
artikel |
13 |
Mechanism of detrimental effects of carbon content on cleavage fracture toughness of low-alloy steel
|
Chen, J. H. |
|
|
32 |
5 |
p. 1081-1091 |
artikel |
14 |
Microstructural size effects in high-strength high-conductivity Cu-Cr-Nb alloys
|
Anderson, Ken R. |
|
|
32 |
5 |
p. 1211-1224 |
artikel |
15 |
On strengthening mechanisms in commercial Nb-Ti hot strip steels
|
Campos, S. S. |
|
|
32 |
5 |
p. 1245-1248 |
artikel |
16 |
Particle formation in the rapidly solidified zone of alloy 600 surface melted by a CO2 laser beam
|
Lim, Yun Soo |
|
|
32 |
5 |
p. 1248-1251 |
artikel |
17 |
Phase equilibria investigations on the aluminum-rich part of the binary system Ti-Al
|
Braun, J. |
|
|
32 |
5 |
p. 1037-1047 |
artikel |
18 |
Spatially resolved X-ray diffraction mapping of phase transformations in the heat-affected zone of carbon-manganese steel arc welds
|
Elmer, John W. |
|
|
32 |
5 |
p. 1175-1187 |
artikel |
19 |
Structures and residual stresses of Cr fibers in Cu-15Cr in-situ composites
|
Sun, Shoujin |
|
|
32 |
5 |
p. 1225-1232 |
artikel |
20 |
Tensile ductility of several commercial aluminum alloys at elevated temperatures
|
Taleff, Eric M. |
|
|
32 |
5 |
p. 1119-1130 |
artikel |
21 |
The evolution of grain boundary character during superplastic deformation of an Al-6 pct Cu-0.4 pct Zr alloy
|
Eddahbi, M. |
|
|
32 |
5 |
p. 1093-1102 |
artikel |
22 |
Ti5Si3 whisker in-situ reinforced TiAl alloys
|
Sun, Fu-Sheng |
|
|
32 |
5 |
p. 1233-1244 |
artikel |