no |
title |
author |
magazine |
year |
volume |
issue |
page(s) |
type |
1 |
A list of Journal Papers on Metals and Strength Problems Published in 2006 and 2007
|
|
|
2008 |
55 |
2 |
p. 180-183 |
article |
2 |
An analysis and assessment of factors causing damage to the waterwall tubes of high-pressure drum boilers
|
Baranov, V. N. |
|
2008 |
55 |
2 |
p. 165-171 |
article |
3 |
An experimental study of the tenacity time of samples made of high-chromium rotor steel for assessing its long-term strength
|
Gladshtein, V. I. |
|
2008 |
55 |
2 |
p. 116-121 |
article |
4 |
A procedure for calculating the swelling of water level and protective means to prevent it from entering into the turbine flow path with the back flow of steam from direct-contact heaters
|
Sukhorukov, Yu. G. |
|
2008 |
55 |
2 |
p. 172-177 |
article |
5 |
Brittle fractures of the drums of high-pressure boilers: Main causes and methods for preventing them
|
Grin’, E. A. |
|
2008 |
55 |
2 |
p. 137-143 |
article |
6 |
Calculating the efficiency of a thermal power station boiler and systems on the basis of exergetic matrices
|
Ivanov, A. P. |
|
2008 |
55 |
2 |
p. 178-179 |
article |
7 |
Development of Russian power engineering in the next 20–30 years
|
Favorskii, O. N. |
|
2008 |
55 |
2 |
p. 95-97 |
article |
8 |
Enlarged thermal deaerators with a horizontal column for large units at nuclear power stations
|
Grigor’ev, G. V. |
|
2008 |
55 |
2 |
p. 161-164 |
article |
9 |
Estimation of remaining service life taking microdamage into account
|
Danyushevskii, I. A. |
|
2008 |
55 |
2 |
p. 112-115 |
article |
10 |
Field experience with the use of forged first-stage rotor blades made of EP800 nickel alloy for the GTE-45 gas turbine
|
Klypina, A. M. |
|
2008 |
55 |
2 |
p. 129-136 |
article |
11 |
Investigation of the fatigue and short-term mechanical properties of 13% chromium steel and titanium alloys after welding or treatment with high-frequency currents as applied to steam-turbine blades
|
Gonserovskii, F. G. |
|
2008 |
55 |
2 |
p. 149-153 |
article |
12 |
Loss of stability of and damage to the coils of platen steam superheaters
|
Bogachev, V. A. |
|
2008 |
55 |
2 |
p. 144-148 |
article |
13 |
Making the tube system’s fitting parts of the low-pressure evaporators used in the heat-recovery boilers of combined-cycle units more resistant to erosion-corrosion wear during operation
|
Tomarov, G. V. |
|
2008 |
55 |
2 |
p. 154-160 |
article |
14 |
Prospects of the development of electricity generation capacities in Russia
|
Makarov, A. A. |
|
2008 |
55 |
2 |
p. 98-111 |
article |
15 |
Regularities pertinent to the cyclic heat resistance of the materials of gas-turbine blades
|
Nikitin, V. I. |
|
2008 |
55 |
2 |
p. 122-128 |
article |