nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Carburization and Stress Profiles Characterized by High-Energy X-ray Diffraction in 316L Austenitic Stainless Steel After Exposure at 500 °C and 600 °C in Carburizing Liquid Sodium
|
Slim, Mohamed Fares |
|
|
96 |
3-4 |
p. 185-199 |
artikel |
2 |
Characterization of PuO/PuCO-Type Phase and its Influence on the Oxidation Kinetics of δ-Plutonium
|
Favart, N. |
|
|
96 |
3-4 |
p. 271-281 |
artikel |
3 |
Comparison Between the Oxidation Behaviors of Ti6242S, Ti6246, TiXT Alloys, and Pure Titanium
|
Vincent, Benjamin |
|
|
96 |
3-4 |
p. 283-294 |
artikel |
4 |
Effectiveness of SiO2/TiO2/Al2O3-Based/TiO2 Coating for Suppressing Circumferential Cracking in Boiler Tubes at Thermal Power Plants
|
Kawase, Makoto |
|
|
96 |
3-4 |
p. 361-372 |
artikel |
5 |
Focus Issue on Unique Materials, Techniques, and Environments
|
Wouters, Yves |
|
|
96 |
3-4 |
p. 183-184 |
artikel |
6 |
High-Temperature Oxidation Behavior of Ti6242S Ti-based Alloy
|
Vande Put, Aurélie |
|
|
96 |
3-4 |
p. 373-384 |
artikel |
7 |
High Temperature Oxidation Kinetics of Shot-Peened and Laser-Shock Peened Ti-Beta-21S
|
Optasanu, V. |
|
|
96 |
3-4 |
p. 257-270 |
artikel |
8 |
Impact of Water Vapor on the High Temperature Oxidation of Wrought and Selective Laser Melted (SLM) AISI 316L
|
Siri, Corentin |
|
|
96 |
3-4 |
p. 347-359 |
artikel |
9 |
In situ Monitoring of the Oxidation of Coated and Uncoated Austenitic Stainless Steels at Temperatures Lower than 600 °C: Part A—Coating Screening
|
Brissonneau, L. |
|
|
96 |
3-4 |
p. 213-230 |
artikel |
10 |
Microstructural Analysis of Zirconia at the Fuel-Cladding Interface in Medium and High Burnup Irradiated Fuel Rods
|
Schneider, C. |
|
|
96 |
3-4 |
p. 295-306 |
artikel |
11 |
Oxidation Behavior of Alx(CoCrFeNi)100-x High-Entropy Alloys Under Thermal-Cycling Conditions
|
Dąbrowa, J. |
|
|
96 |
3-4 |
p. 307-321 |
artikel |
12 |
Oxidation of Mo-Si-B Alloys and Coatings in a Water Vapor Environment
|
Perepezko, J. H. |
|
|
96 |
3-4 |
p. 323-332 |
artikel |
13 |
Pre-Oxidation to Improve Liquid Metal Compatibility
|
Pint, Bruce A. |
|
|
96 |
3-4 |
p. 231-240 |
artikel |
14 |
Should Gold Marker or TEM-ASTAR Characterization Be Used to Determine Oxide Growth Direction?
|
Latu-Romain, L. |
|
|
96 |
3-4 |
p. 201-211 |
artikel |
15 |
The Effect of Al on the Formation of a CrTaO4 Layer in Refractory High Entropy Alloys Ta-Mo-Cr-Ti-xAl
|
Schellert, S. |
|
|
96 |
3-4 |
p. 333-345 |
artikel |
16 |
The Effect of Cu Content and Surface Finish on the Metal Dusting Resistance of Additively Manufactured NiCu Alloys
|
Jahns, Katrin |
|
|
96 |
3-4 |
p. 241-256 |
artikel |