nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Air Oxidation of Ni–Ti Alloys at 650–850°C
|
Zeng, C.L. |
|
2002 |
58 |
1-2 |
p. 171-184 |
artikel |
2 |
Corrosion Behavior of a Sputtered K38G Nanocrystalline Coating with a Solid NaCl Deposit in Wet Oxygen at 600 to 700°C
|
Wang, Fuhui |
|
2002 |
58 |
1-2 |
p. 185-195 |
artikel |
3 |
Effect of Cycle Frequency on High-Temperature Oxidation Behavior of Alumina-Forming Alloys
|
Pint, B.A. |
|
2002 |
58 |
1-2 |
p. 73-101 |
artikel |
4 |
Effect of Ternary Elements on the Oxidation Behavior of Aluminized TiAl Alloys
|
Jung, Hwan Gyo |
|
2002 |
58 |
1-2 |
p. 197-216 |
artikel |
5 |
Effects of Laser Surface Modification of Nimonic with Aluminum on Oxidation Behavior
|
Rodriguez, G.P. |
|
2002 |
58 |
1-2 |
p. 235-248 |
artikel |
6 |
Investigation of Metal-Dusting Mechanism in Fe-Base Alloys Using Raman Spectroscopy, X-Ray Diffraction, and Electron Microscopy
|
Zeng, Z. |
|
2002 |
58 |
1-2 |
p. 147-170 |
artikel |
7 |
Mechanism of Chromium Oxidation in SO2 at 3 × 104 Pa and 105 Pa
|
Gilewicz-Wolter, J. |
|
2002 |
58 |
1-2 |
p. 217-233 |
artikel |
8 |
Metal Dusting of Fe–Cr and Fe–Ni–Cr Alloys Under Cyclic Conditions
|
Toh, C.H. |
|
2002 |
58 |
1-2 |
p. 1-21 |
artikel |
9 |
Oxidation Resistance of Ti5Si3 and Ti5Si3Zx at 1000°C (Z = C, N, or O)
|
Williams, J.J. |
|
2002 |
58 |
1-2 |
p. 57-71 |
artikel |
10 |
Role of Growth Stresses on the Structure of Oxide Scales on Nickel at 800 and 900°C
|
Przybilla, W. |
|
2002 |
58 |
1-2 |
p. 103-145 |
artikel |
11 |
TEM Study of Scale Microstructures Formed on Ni–10Cr and Ni–10Cr–5Al Alloys with and Without Y Addition
|
Ul-Hamid, A. |
|
2002 |
58 |
1-2 |
p. 41-56 |
artikel |
12 |
TEM Study of the Effect of Y on the Scale Microstructures of Cr2O3- and Al2O3-Forming Alloys
|
Ul-Hamid, A. |
|
2002 |
58 |
1-2 |
p. 23-40 |
artikel |