nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Acoustic emission due to deformation twinning in titanium and Ti6Al4V alloy
|
Tanaka, H. |
|
1975 |
9 |
7 |
p. 777-780 4 p. |
artikel |
2 |
7. An electron microscopy study of the precipitation in an invar-3.31 at .% Sn alloy
|
Nissan, S.I. |
|
1975 |
9 |
7 |
p. xxx-xxxi nvt p. |
artikel |
3 |
An experimental method for demonstrating the heterogeneity of short range ordered phases (α-CuAl)
|
Veith, G. |
|
1975 |
9 |
7 |
p. 737-742 6 p. |
artikel |
4 |
A technique for determination of hydrogen content
|
Berkowitz, B.J. |
|
1975 |
9 |
7 |
p. 803-806 4 p. |
artikel |
5 |
Comment on “the Watson-McDougall shear: proof that Widmanstatten ferrite cannot grow martensitically”
|
McDougall, P.G. |
|
1975 |
9 |
7 |
p. 713-715 3 p. |
artikel |
6 |
Comparative measurements of the recrystallization energy by different calorimeters
|
Gottstein, G. |
|
1975 |
9 |
7 |
p. 791-796 6 p. |
artikel |
7 |
9. Creep cavitation failure in copper subject to biaxial stress systems at 250°C
|
Kelly, D.A. |
|
1975 |
9 |
7 |
p. xxxi- 1 p. |
artikel |
8 |
19. Cyclic deformation of commercial-purity titanium
|
Stevenson, R. |
|
1975 |
9 |
7 |
p. xxxiv- 1 p. |
artikel |
9 |
Decomposition of austenite in an iron-cobalt-molybdenum alloy
|
Musiol, C. |
|
1975 |
9 |
7 |
p. 693-696 4 p. |
artikel |
10 |
Diffusion of 114mIn in NiAl
|
Lutze-Birk, A. |
|
1975 |
9 |
7 |
p. 761-765 5 p. |
artikel |
11 |
Direct observation of 〈110〉{110} slip in FCC single crystals of a nickel base superalloy
|
Carry, C. |
|
1975 |
9 |
7 |
p. 731-736 6 p. |
artikel |
12 |
2. Effect of solute and orientation on the mobility of near-coincidence tilt boundaries in high-purity aluminum
|
Demianczuk, D.W. |
|
1975 |
9 |
7 |
p. xxix- 1 p. |
artikel |
13 |
10. Elastic-plastic memory and kinematic-type hardening
|
Asaro, R.J. |
|
1975 |
9 |
7 |
p. xxxi- 1 p. |
artikel |
14 |
Etude par microscopie electronique de la cinetique de precipitation dans un alliage de cuivre a 2, 1 % de fer
|
Borrelly, R. |
|
1975 |
9 |
7 |
p. 747-752 6 p. |
artikel |
15 |
15. Field ion microscope studies of solute atoms in dilute Pt alloys I. Contrast due to Au, Ni and W atoms
|
Chen, C.G. |
|
1975 |
9 |
7 |
p. xxxiii- 1 p. |
artikel |
16 |
16. Field ion microscope studies of solute atoms in dilute Pt alloys. II. Distributions and interactions of Au and Ni atoms
|
Chen, C.G. |
|
1975 |
9 |
7 |
p. xxxiii- 1 p. |
artikel |
17 |
Frottement interieur du niobium apres deformation a basse temperature
|
Ferron, G. |
|
1975 |
9 |
7 |
p. 697-704 8 p. |
artikel |
18 |
High tetragonality of the thermoelastic Fe3Pt martensite and small volume change during the transformation
|
Tadaki, T. |
|
1975 |
9 |
7 |
p. 771-776 6 p. |
artikel |
19 |
1. Influence de l'environment sur les facies de rupture par fatigue d'eprouvettes monocristallines et polycristallines d'alliage aluminium-cuivre 4%
|
Bouchet, B. |
|
1975 |
9 |
7 |
p. xxix- 1 p. |
artikel |
20 |
Influence de l'etat structural sur les valeurs, a temperature ambiante des constantes elastiques de Ni3Fe
|
Turchi, P. |
|
1975 |
9 |
7 |
p. 797-800 4 p. |
artikel |
21 |
Influence of phosphorus upon growth of aluminium and silicon nitrides in ferrite
|
Pope, M. |
|
1975 |
9 |
7 |
p. 717-721 5 p. |
artikel |
22 |
Inhibition of hydrogen environment embrittlement by SO2
|
Jacobs, A.J. |
|
1975 |
9 |
7 |
p. 767-769 3 p. |
artikel |
23 |
12. Interpretations for thermomigration results in aluminum and aluminum alloys
|
McKee, R.A. |
|
1975 |
9 |
7 |
p. xxxii- 1 p. |
artikel |
24 |
Loss of lattice rigidity in iron-nitrogen austenite
|
De Cristofaro, Nicholas |
|
1975 |
9 |
7 |
p. 781-785 5 p. |
artikel |
25 |
4. Modelling of rearrangement processes in liquid phase sintering
|
Huppmann, W.J. |
|
1975 |
9 |
7 |
p. xxx- 1 p. |
artikel |
26 |
14. On liesegang bands in internally oxidized AgCd-based ternary alloys
|
vanRooijen, V.A. |
|
1975 |
9 |
7 |
p. xxxii- 1 p. |
artikel |
27 |
On the efficiency of the shape memory effect for energy conversion
|
Wayman, C.M. |
|
1975 |
9 |
7 |
p. 757-760 4 p. |
artikel |
28 |
5. Polycrystalline strengthening
|
Margolin, H. |
|
1975 |
9 |
7 |
p. xxx- 1 p. |
artikel |
29 |
Prediction of irradiation creep from microstructural data
|
Wolfer, W.G. |
|
1975 |
9 |
7 |
p. 801-802 2 p. |
artikel |
30 |
Resistivity decay in quenched impure aluminium
|
Sanderson, S.J. |
|
1975 |
9 |
7 |
p. 753-755 3 p. |
artikel |
31 |
6. Rolling and bending deformation of NiPdP metal glasses
|
Takayama, S. |
|
1975 |
9 |
7 |
p. xxx- 1 p. |
artikel |
32 |
Size effect on recovery process of quenched-in-hydrogen in nickel
|
Tada, Masato |
|
1975 |
9 |
7 |
p. 743-745 3 p. |
artikel |
33 |
8. Some correlations between the athermal and the isothermal modes of martensitic transformation
|
Gupta, S.K. |
|
1975 |
9 |
7 |
p. xxxi- 1 p. |
artikel |
34 |
20. Static distortions and resistivity due to interstitials
|
McIntire, W.R. |
|
1975 |
9 |
7 |
p. xxxiv- 1 p. |
artikel |
35 |
3. Supercoolings observed for droplets of tin, alloys of tin, and certain other pure metals
|
Rasmussen, D.H. |
|
1975 |
9 |
7 |
p. xxix-xxx nvt p. |
artikel |
36 |
The dependence of the threshold stress intensity factor on the cyclic stress ratio in fatigue of ferritic-pearlitic steels
|
Masounaye, J. |
|
1975 |
9 |
7 |
p. 723-730 8 p. |
artikel |
37 |
11. The effect of order on the low cycle fatigue response of Cu3Au single crystals
|
Chien, K.H. |
|
1975 |
9 |
7 |
p. xxxi-xxxii nvt p. |
artikel |
38 |
21. The influence of crystallographic orientation on fatigue crack growth in strongly textured Ti6Al4V
|
Bowen, A.W. |
|
1975 |
9 |
7 |
p. xxxiv- 1 p. |
artikel |
39 |
18. The interaction between grain growth and recrystallization in an AlZnMg-alloy
|
Nes, K.J. |
|
1975 |
9 |
7 |
p. xxxiii-xxxiv nvt p. |
artikel |
40 |
13. Theory of surface enrichment and surface disorder effects in binary alloys
|
Binder, K. |
|
1975 |
9 |
7 |
p. xxxii- 1 p. |
artikel |
41 |
Thermodynamic investigations of group IV chalcogenides
|
Shamsuddin, |
|
1975 |
9 |
7 |
p. 807-809 3 p. |
artikel |
42 |
17. The tin-iron eutectic
|
Connolly, J.J. |
|
1975 |
9 |
7 |
p. xxxiii- 1 p. |
artikel |
43 |
The Watson-McDougall shear: Proof that Widmanstatten ferrite cannot grow martensitically
|
Aaronson, H.I. |
|
1975 |
9 |
7 |
p. 705-712 8 p. |
artikel |
44 |
Young's modulus and hardness of metallic (Pd1−xNix).835Si.165 glasses
|
Chen, H.S. |
|
1975 |
9 |
7 |
p. 787-789 3 p. |
artikel |