nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Aluminide coatings on TiAl compound
|
Mabuchi, Hiroshi |
|
1989 |
23 |
5 |
p. 685-689 5 p. |
artikel |
2 |
A modification on the portevin-le chatelier effect of substitutional FCC alloys
|
Chen, M.C. |
|
1989 |
23 |
5 |
p. 655-658 4 p. |
artikel |
3 |
An FCC-based special point ordered structure generated by tiling
|
Kulkarni, U.D. |
|
1989 |
23 |
5 |
p. 811-814 4 p. |
artikel |
4 |
Anomalies in the deformation characteristics of intermetallic TiAl: Theoretical models
|
Greenberg, B.A. |
|
1989 |
23 |
5 |
p. 631-636 6 p. |
artikel |
5 |
A transition of microstructure in heavily cold rolled 70:30 brass
|
Yeung, W.Y. |
|
1989 |
23 |
5 |
p. 617-620 4 p. |
artikel |
6 |
Combined mode I - mode III fracture toughness of a high carbon steel
|
Manoharan, M. |
|
1989 |
23 |
5 |
p. 763-766 4 p. |
artikel |
7 |
Comment on “the strain rate sensitivity during serrated yielding”
|
Kubin, L.P. |
|
1989 |
23 |
5 |
p. 815-817 3 p. |
artikel |
8 |
Crystallization of glassy Pd80Si20 studied by perturbed angular correlation
|
Schumacher, G. |
|
1989 |
23 |
5 |
p. 625-630 6 p. |
artikel |
9 |
Crystallographic texture of melt-spun AlMn based and AlLiCu icosahedral quasicrystals
|
Sugawara, T. |
|
1989 |
23 |
5 |
p. 711-716 6 p. |
artikel |
10 |
Deformations of materials exhibiting noncoaxiality and finite rotations
|
Zbib, Hussein M. |
|
1989 |
23 |
5 |
p. 789-794 6 p. |
artikel |
11 |
Dislocation densities as determined by tem in [100] and [111] Cu Mn crystals
|
Neuhaus, R. |
|
1989 |
23 |
5 |
p. 779-784 6 p. |
artikel |
12 |
Dislocation densities in [001]-orientated Cu -Mn single crystals deformed in tension. Determination by X-ray diffraction line broadening
|
Hilscher, A. |
|
1989 |
23 |
5 |
p. 785-788 4 p. |
artikel |
13 |
Dispersoids in rapidly solidified B2 nickel aluminides
|
Jha, S.C. |
|
1989 |
23 |
5 |
p. 805-810 6 p. |
artikel |
14 |
Editorial: Software survey section
|
|
|
1989 |
23 |
5 |
p. I-III nvt p. |
artikel |
15 |
Effect of an electric field on the superplasticity of 7475 Al
|
Conrad, H. |
|
1989 |
23 |
5 |
p. 697-702 6 p. |
artikel |
16 |
Effect of heat treatment on the structure, properties and fracture of Nd: YAG laser welded Ti-14.8 wt% Al-21.3 wt% Nb
|
Baeslack III, W.A. |
|
1989 |
23 |
5 |
p. 717-720 4 p. |
artikel |
17 |
Effect of particle oxidation on age hardening of AlSiMg/SiC composites
|
Ribes, H. |
|
1989 |
23 |
5 |
p. 705-709 5 p. |
artikel |
18 |
Energy loss mechanisms in the erosion of cemented tungsten carbide
|
Freinkel, D.M. |
|
1989 |
23 |
5 |
p. 659-664 6 p. |
artikel |
19 |
Erratum
|
|
|
1989 |
23 |
5 |
p. 819- 1 p. |
artikel |
20 |
Fatigue crack propagation behavior of 63Sn-37Pb solder
|
Liaw, P.K. |
|
1989 |
23 |
5 |
p. 747-752 6 p. |
artikel |
21 |
Inhibition of grain growth by second phase particles: Three dimensional Monte Carlo computer simulations
|
Anderson, M.P. |
|
1989 |
23 |
5 |
p. 753-758 6 p. |
artikel |
22 |
In-situ imaging of creep cavities by synchrotron microradiography
|
Dobbyn, R.C. |
|
1989 |
23 |
5 |
p. 621-623 3 p. |
artikel |
23 |
Melting behavior of SnBi alloy droplets during continuous heating
|
Allen, W.P. |
|
1989 |
23 |
5 |
p. 643-648 6 p. |
artikel |
24 |
Microstructural investigation of hardfacing weld deposit obtained from CrB paste
|
Kr.Ray, Santanu |
|
1989 |
23 |
5 |
p. 737-742 6 p. |
artikel |
25 |
Nature of boron and nitrogen superficial “segregation” on the FeNi 36 alloys
|
Saindrenan, G. |
|
1989 |
23 |
5 |
p. 665-669 5 p. |
artikel |
26 |
On the achievement of strength at high temperature in binary alloys
|
Louat, N.P. |
|
1989 |
23 |
5 |
p. 721-726 6 p. |
artikel |
27 |
On the kinetics of recrystallisation in cold worked metals
|
Hutchinson, Bevis |
|
1989 |
23 |
5 |
p. 671-676 6 p. |
artikel |
28 |
Prediction of slip transfer mechanisms across grain boundaries
|
Lee, T.C. |
|
1989 |
23 |
5 |
p. 799-803 5 p. |
artikel |
29 |
Quasicrystalline phases in AlCuCo alloy
|
Zhang, Z. |
|
1989 |
23 |
5 |
p. 767-772 6 p. |
artikel |
30 |
Research on the cause of surface crack tip plastic zone growth in stress corrosion cracking
|
Lan, Yun |
|
1989 |
23 |
5 |
p. 677-683 7 p. |
artikel |
31 |
Role de l'energie de faute d'empilement dans le choix des equations constitutives
|
Blanchard, P |
|
1989 |
23 |
5 |
p. 733-736 4 p. |
artikel |
32 |
Simulation of lineal roughness index of random curvature fracture profiles
|
Ray, K.K. |
|
1989 |
23 |
5 |
p. 759-762 4 p. |
artikel |
33 |
Stability of the icosahedral phase in Mn-Ti alloys
|
Holzer, J.C. |
|
1989 |
23 |
5 |
p. 691-695 5 p. |
artikel |
34 |
Surface oxidation and ductility loss in boron-doped Ni3Al at 760°C
|
Takeyama, M. |
|
1989 |
23 |
5 |
p. 727-731 5 p. |
artikel |
35 |
The brittle-ductile transition in silicon: The influence of pre-existing dislocation arrangements
|
Warren, P.D. |
|
1989 |
23 |
5 |
p. 637-642 6 p. |
artikel |
36 |
The distribution of grain boundary plane orientations in a metastable grain aggregate
|
Randle, Valerie |
|
1989 |
23 |
5 |
p. 773-778 6 p. |
artikel |
37 |
The electron diffraction patterns(EDPS) of Nd1+ϵ Fe4B4 compounds
|
Zhibo, Zhao |
|
1989 |
23 |
5 |
p. 743-746 4 p. |
artikel |
38 |
The iron-neodymium phase diagram
|
Faudot, F. |
|
1989 |
23 |
5 |
p. 795-798 4 p. |
artikel |
39 |
The oxidation behaviour of amorphous Fe40Ni40B20
|
Wei, Gao |
|
1989 |
23 |
5 |
p. 649-654 6 p. |
artikel |
40 |
Void nucleation and strain hardening
|
Vijayaraghavan, T.V. |
|
1989 |
23 |
5 |
p. 703-704 2 p. |
artikel |