nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Advanced Tube Inspection System
|
Iwamoto, K. |
|
2005 |
49 |
7-8 |
p. 33-36 |
artikel |
2 |
An Evaluation Method for Laser Weld Metal Toughness by Side-Notched Charpy Test
|
Hagihara, Y. |
|
2005 |
49 |
7-8 |
p. 21-27 |
artikel |
3 |
Assessment of Hydrogen Cracking Risk in Multipass Weld Metal of 2.25Cr-1Mo-0.25V-TiB (T24) Boiler Steel
|
Nevasmaa, P. |
|
2005 |
49 |
7-8 |
p. 45-58 |
artikel |
4 |
Coming Events
|
|
|
2005 |
49 |
7-8 |
p. 78-79 |
artikel |
5 |
Eddy Current Non-Destructive Surface Testing of Weld Coated with Anticorrosion Painting
|
Hoshikawa, H. |
|
2005 |
49 |
7-8 |
p. 28-32 |
artikel |
6 |
Effect of Repair Welding on the Creep Rupture Strength of an Aged Weldment
|
Ozaki, M. |
|
2005 |
49 |
7-8 |
p. 67-72 |
artikel |
7 |
IIW International Congress “Frontiers of Welding Science and Technology” Mumbai (India) 16–19 February 2005
|
|
|
2005 |
49 |
7-8 |
p. 5-6 |
artikel |
8 |
IIW International Congres “Welding and Joining 2005: Frontiers of Materials Joining” Tel Aviv (Israel) 25–27 January 2005
|
|
|
2005 |
49 |
7-8 |
p. 3-4 |
artikel |
9 |
Improvement of Creep Strength of Advanced Ferritic Steel Welded Joints
|
Abe, F. |
|
2005 |
49 |
7-8 |
p. 59-66 |
artikel |
10 |
Investigation of Dissolution and Precipitation Behaviours of Precipitates in Welded Joints of High Cr Ferritic Heat Resistant Steels
|
Li, D. J. |
|
2005 |
49 |
7-8 |
p. 7-15 |
artikel |
11 |
Manufacturing with Lasers, Developments and Opportunities
|
Booth, G. S. |
|
2005 |
49 |
7-8 |
p. 16-20 |
artikel |
12 |
Repair of Stress Corrosion Cracking in Overlaying of Inconel 182 by Laser Surface Melting
|
Bao, G. |
|
2005 |
49 |
7-8 |
p. 37-44 |
artikel |
13 |
Vibration Welding of Carpet to Polypropylene Substrate
|
Wu, C. Y. |
|
2005 |
49 |
7-8 |
p. 73-77 |
artikel |