nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A thermodynamics model for solder profile evolution
|
Gao, Y.X. |
|
2000 |
48 |
4 |
p. 863-874 12 p. |
artikel |
2 |
Crystallographic aspects of deformation twinning and consequences for plastic deformation processes in γ-TiAl
|
Skrotzki, B. |
|
2000 |
48 |
4 |
p. 851-862 12 p. |
artikel |
3 |
Decomposition of martensite by discontinuous-like precipitation reaction in an Fe–17Cr–0.5C alloy
|
Shtansky, D.V |
|
2000 |
48 |
4 |
p. 969-983 15 p. |
artikel |
4 |
Deformation-induced defects controlling fracture toughness of steel revealed by tritium desorption behaviors
|
Nagumo, M |
|
2000 |
48 |
4 |
p. 943-951 9 p. |
artikel |
5 |
Determination of the chemical width of grain boundaries of boron- and carbon-doped hot-pressed β-SiC by HAADF imaging and ELNES line-profile
|
Kaneko, K. |
|
2000 |
48 |
4 |
p. 903-910 8 p. |
artikel |
6 |
Editorial
|
Gschneidner Jr, Karl A |
|
2000 |
48 |
4 |
p. vii- 1 p. |
artikel |
7 |
Grain boundaries in dielectric and mixed-conducting ceramics
|
Waser, R. |
|
2000 |
48 |
4 |
p. 797-825 29 p. |
artikel |
8 |
Influence of the metal particle size on toughness of Al2O3/Mo composite
|
Sbaizero, O |
|
2000 |
48 |
4 |
p. 985-992 8 p. |
artikel |
9 |
Instability mechanisms in lamellar microstructures
|
Sharma, G. |
|
2000 |
48 |
4 |
p. 875-889 15 p. |
artikel |
10 |
Modeling the effect of temperature on the wear resistance of metals reinforced with ceramic particles
|
Rodrı́guez, J |
|
2000 |
48 |
4 |
p. 993-1003 11 p. |
artikel |
11 |
Nanocrystalline Ni–3.6 at.% P and its transformation sequence studied by atom-probe field-ion microscopy
|
Hentschel, Th |
|
2000 |
48 |
4 |
p. 933-941 9 p. |
artikel |
12 |
Nanoparticles from compounds with layered structures
|
Vollath, D. |
|
2000 |
48 |
4 |
p. 953-967 15 p. |
artikel |
13 |
Permeation of hydrogen in Ni-based superalloy CMSX-4
|
Rothová, V. |
|
2000 |
48 |
4 |
p. 827-833 7 p. |
artikel |
14 |
Rapid solution hardening at elevated temperatures by substitutional Re alloying in MoSi2
|
Misra, A. |
|
2000 |
48 |
4 |
p. 925-932 8 p. |
artikel |
15 |
Steady-state creep of a particulate SiC/6061 Al composite
|
Wakashima, K |
|
2000 |
48 |
4 |
p. 891-901 11 p. |
artikel |
16 |
Structural stability of the Laves phase Cr2Ta in a two-phase Cr–Cr2Ta alloy
|
Kumar, K.S. |
|
2000 |
48 |
4 |
p. 911-923 13 p. |
artikel |
17 |
Thermal behavior during droplet-based deposition
|
Xu, Q |
|
2000 |
48 |
4 |
p. 835-849 15 p. |
artikel |