nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A general morphological approach of sintering kinetics: application to WC–Co solid phase sintering
|
Missiaen, J.-M. |
|
1998 |
46 |
11 |
p. 3985-3993 9 p. |
artikel |
2 |
Computer simulation of morphological evolution and coarsening kinetics of δ′ (Al3Li) precipitates in Al–Li alloys
|
Poduri, R. |
|
1998 |
46 |
11 |
p. 3915-3928 14 p. |
artikel |
3 |
Control of grain growth using intergranular silicate phases in cubic yttria stabilized zirconia
|
Sharif, A.A. |
|
1998 |
46 |
11 |
p. 3863-3872 10 p. |
artikel |
4 |
Crystallography of spheroidite and tempered martensite
|
Zhang, M.-X. |
|
1998 |
46 |
11 |
p. 4081-4091 11 p. |
artikel |
5 |
Current density and line width effects in electromigration: a new damage-based lifetime model
|
Kraft, O. |
|
1998 |
46 |
11 |
p. 3733-3743 11 p. |
artikel |
6 |
Diffusional back flows during electromigration
|
Blech, I.A. |
|
1998 |
46 |
11 |
p. 3717-3723 7 p. |
artikel |
7 |
Discussion
|
|
|
1998 |
46 |
11 |
p. 3755-3760 6 p. |
artikel |
8 |
Effect of inclusion morphology on the densification of powder composites
|
Delie, F. |
|
1998 |
46 |
11 |
p. 3905-3913 9 p. |
artikel |
9 |
Effects of substrate cooling in hard magnetic disk sputtering process on protective overcoat and magnetic layer properties
|
Anoikin, E.V. |
|
1998 |
46 |
11 |
p. 3787-3791 5 p. |
artikel |
10 |
Evolution of microstructures resulting from dendrite growth in undercooled Fe–Cr–Ni melts
|
Moir, S.A. |
|
1998 |
46 |
11 |
p. 4029-4036 8 p. |
artikel |
11 |
Fabrication of film heads with high moment materials
|
Jones Jr, R.E. |
|
1998 |
46 |
11 |
p. 3805-3812 8 p. |
artikel |
12 |
Flow behavior of PST and fully lamellar polycrystals of Ti–48Al in the microstrain regime
|
Parthasarathy, T.A. |
|
1998 |
46 |
11 |
p. 4005-4016 12 p. |
artikel |
13 |
High-strain-rate deformation of granular silicon carbide
|
Shih, C.J. |
|
1998 |
46 |
11 |
p. 4037-4065 29 p. |
artikel |
14 |
High strain rate superplasticity in metal matrix composites: the role of load transfer
|
Li, Y. |
|
1998 |
46 |
11 |
p. 3937-3948 12 p. |
artikel |
15 |
High temperature plastic deformation of multilayered YTZP/ZTA composites obtained by tape casting
|
Jiménez-Melendo, M. |
|
1998 |
46 |
11 |
p. 3995-4004 10 p. |
artikel |
16 |
Internal stresses and strains in coherent multilayers
|
Shoykhet, B. |
|
1998 |
46 |
11 |
p. 3761-3766 6 p. |
artikel |
17 |
Kinetics of stress relaxation caused by the combination of interfacial sliding and diffusion: two-dimensional analysis
|
Onaka, S. |
|
1998 |
46 |
11 |
p. 3821-3828 8 p. |
artikel |
18 |
Liquidus temperatures and solidification behavior in the copper–niobium system
|
Li, D |
|
1998 |
46 |
11 |
p. 3849-3855 7 p. |
artikel |
19 |
Materials issues in design and performance of piezoelectric actuators: an overview
|
Uchino, K. |
|
1998 |
46 |
11 |
p. 3745-3753 9 p. |
artikel |
20 |
Mechanical behavior of an Fe–40Al–0.6C alloy
|
Pang, L. |
|
1998 |
46 |
11 |
p. 4017-4028 12 p. |
artikel |
21 |
Micro/nanoscale friction and wear mechanisms of thin films using atomic force and friction force microscopy
|
Bhushan, B |
|
1998 |
46 |
11 |
p. 3793-3804 12 p. |
artikel |
22 |
Microstructures and basic magnetic properties of Co-based epitaxial magneticthin films
|
Futamoto, M. |
|
1998 |
46 |
11 |
p. 3777-3786 10 p. |
artikel |
23 |
Microstructures and mechanical properties of rapidly solidified high strength Al–Ni based alloys
|
Guo, J.Q |
|
1998 |
46 |
11 |
p. 3829-3838 10 p. |
artikel |
24 |
Misorientation effects on discontinuous precipitation in Al–Ag–Ga
|
Hirth, S |
|
1998 |
46 |
11 |
p. 3975-3984 10 p. |
artikel |
25 |
Modelling of reaustenitization from the pearlite structure in steel
|
Jacot, A. |
|
1998 |
46 |
11 |
p. 3949-3962 14 p. |
artikel |
26 |
Modification of interdendritic convection in directional solidification by a uniform magnetic field
|
Lehmann, P. |
|
1998 |
46 |
11 |
p. 4067-4079 13 p. |
artikel |
27 |
Orientation dependence of creep of Ni3Al at intermediate temperature
|
Zhu, W.H. |
|
1998 |
46 |
11 |
p. 3873-3881 9 p. |
artikel |
28 |
Preface to the Special Section on ``Coupled Property Issues in Integrated Microstructures''
|
Krishnan, K.M. |
|
1998 |
46 |
11 |
p. 3715- 1 p. |
artikel |
29 |
Stable state of interconnect under temperature change and electric current
|
Suo, Z. |
|
1998 |
46 |
11 |
p. 3725-3732 8 p. |
artikel |
30 |
Stress singularity near the crack-tip in silicon carbide: investigation by atomic force microscopy
|
Kinoshita, T. |
|
1998 |
46 |
11 |
p. 3963-3974 12 p. |
artikel |
31 |
The effect of nitrogenation on GMR and microstructures of granular (Ni0.8Fe0.2)20Ag80 thin films
|
Oh, T.S |
|
1998 |
46 |
11 |
p. 3813-3820 8 p. |
artikel |
32 |
The effect of the microstructure on the superplasticity of a duplex stainless steel
|
Sagradi, M |
|
1998 |
46 |
11 |
p. 3857-3862 6 p. |
artikel |
33 |
The effects of cell face curvature and corrugations on the stiffness and strength of metallic foams
|
Simone, A.E. |
|
1998 |
46 |
11 |
p. 3929-3935 7 p. |
artikel |
34 |
The precipitation sequence in Al–Mg–Si alloys
|
Edwards, G.A. |
|
1998 |
46 |
11 |
p. 3893-3904 12 p. |
artikel |
35 |
The strength of Al2O3/SiC nanocomposites after grinding and annealing
|
Wu, H.Z |
|
1998 |
46 |
11 |
p. 3839-3848 10 p. |
artikel |
36 |
Unified thermodynamic analysis of the stress-assisted γ→ε martensitic transformation in Fe–Mn–Si alloys
|
Andersson, M. |
|
1998 |
46 |
11 |
p. 3883-3891 9 p. |
artikel |
37 |
X-ray optical multilayers: microstructure limits on reflectivity at ultra-short periods
|
Walton, C.C |
|
1998 |
46 |
11 |
p. 3767-3775 9 p. |
artikel |