nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A novel process for breakdown forging of coarse-grain intermetallic alloys
|
Semiatin, S.L. |
|
1993 |
29 |
9 |
p. 1235-1240 6 p. |
artikel |
2 |
Comment on “The ductile-brittle transition of a zirconium alloy due to hydrogen” by J. H. Huang, S. P. Huang and C. S. Ho
|
Bai, J.B. |
|
1993 |
29 |
9 |
p. 1259-1260 2 p. |
artikel |
3 |
Densification of sintered porous metal under hydrostatic pressure
|
Han, Heung Nam |
|
1993 |
29 |
9 |
p. 1211-1216 6 p. |
artikel |
4 |
Formation, propagation of bands and chaos in jerky flow
|
Ananthakrishna, G. |
|
1993 |
29 |
9 |
p. 1183-1188 6 p. |
artikel |
5 |
Hydrogen transport behavior of timetal-21S alloy
|
Sankaran, Sankara N. |
|
1993 |
29 |
9 |
p. 1247-1252 6 p. |
artikel |
6 |
Improvement of fracture toughness of forging steels microalloyed with titanium by accelerated cooling after hot working
|
Linaza, M.A. |
|
1993 |
29 |
9 |
p. 1217-1222 6 p. |
artikel |
7 |
Introductory remarks to the viewpoint set on propagative plastic instabilities
|
Estrin, Y. |
|
1993 |
29 |
9 |
p. 1147-1150 4 p. |
artikel |
8 |
Modelling of propagative plastic instabilities
|
Hähner, Peter |
|
1993 |
29 |
9 |
p. 1171-1176 6 p. |
artikel |
9 |
Observation of lüders bands in single crystals
|
Neuhäuser, H. |
|
1993 |
29 |
9 |
p. 1151-1157 7 p. |
artikel |
10 |
On the anomalous creep behaviour of an XD Al-TiB2 composite
|
Pandey, A.B. |
|
1993 |
29 |
9 |
p. 1199-1204 6 p. |
artikel |
11 |
Preliminary investigation of the kinetics of primary creep of a two phase gamma TiAl alloy
|
Hayes, R.W. |
|
1993 |
29 |
9 |
p. 1229-1233 5 p. |
artikel |
12 |
Propagating pattern selection in the Portevin-Le Chatelier effect
|
Jeanclaude, Véronique |
|
1993 |
29 |
9 |
p. 1177-1182 6 p. |
artikel |
13 |
Propagative instabilities: An experimental view
|
McCormick, P.G. |
|
1993 |
29 |
9 |
p. 1159-1164 6 p. |
artikel |
14 |
Reinforcement phase stability during ageing of an aluminium alloy/yttria-stabilised zirconia composite
|
Lewis, C.A. |
|
1993 |
29 |
9 |
p. 1189-1194 6 p. |
artikel |
15 |
Static versus propagative plastic strain localisations
|
Bréchet, Y.J.M. |
|
1993 |
29 |
9 |
p. 1165-1170 6 p. |
artikel |
16 |
Steady state behaviour of alloy 800H under cyclic deformation
|
Estrin, Y. |
|
1993 |
29 |
9 |
p. 1223-1228 6 p. |
artikel |
17 |
Suppression of environmental embrittlement in boron-free Ni3Al by unidirectional solidification
|
Nishimura, C. |
|
1993 |
29 |
9 |
p. 1205-1209 5 p. |
artikel |
18 |
Surface analysis of an aluminium metal matrix composite
|
Manzano-Ramirez, A. |
|
1993 |
29 |
9 |
p. 1241-1246 6 p. |
artikel |
19 |
Surface modification of powder materials and room temperature activation of V, Ni and TiFe
|
Lü, Manqi |
|
1993 |
29 |
9 |
p. 1253-1258 6 p. |
artikel |
20 |
Temperature and strain rate dependence of hot ductility in worked free-cutting brass
|
Vasconcelos, W.L. |
|
1993 |
29 |
9 |
p. 1195-1198 4 p. |
artikel |