nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Aging behavior of powder metallurgy composite
|
Lee, Huei-Long |
|
1992 |
26 |
11 |
p. 1723-1726 4 p. |
artikel |
2 |
A model for crack growth behaviour of macroscopically deflected fatigue cracks
|
Kamat, S.V. |
|
1992 |
26 |
11 |
p. 1713-1718 6 p. |
artikel |
3 |
Comments on “Measurement of grain size using the circle intercept method”
|
Voort, G.F.Vander |
|
1992 |
26 |
11 |
p. 1785-1790 6 p. |
artikel |
4 |
Cracking behavior of FeAl (40 at % Al) alloys during cutting operations
|
Ferguson, Patrick A. |
|
1992 |
26 |
11 |
p. 1669-1674 6 p. |
artikel |
5 |
Deformation of nanoscale cermets
|
Evans, A.G. |
|
1992 |
26 |
11 |
p. 1675-1680 6 p. |
artikel |
6 |
Ductility improvement on Al67Ti25Mn8 intermetallic alloy via hot-working
|
Chen, Xiaofu |
|
1992 |
26 |
11 |
p. 1775-1778 4 p. |
artikel |
7 |
Effect of heat treatment and thermal cycling on transformation temperatures of ductile Cu-Al-Ni-Mn-B alloys
|
Morris, M.A. |
|
1992 |
26 |
11 |
p. 1663-1668 6 p. |
artikel |
8 |
Effect of microstructure on hot deformation in duplex stainless steels
|
Maehara, Yasuhiro |
|
1992 |
26 |
11 |
p. 1701-1706 6 p. |
artikel |
9 |
Environmental effect on mechanical properties of L12-ordered (Fe22Co78)3V
|
Miura, S. |
|
1992 |
26 |
11 |
p. 1753-1758 6 p. |
artikel |
10 |
Fatigue crack growth rates in arctic-grade line pipe steel at high ΔK
|
Wake, C.R. |
|
1992 |
26 |
11 |
p. 1693-1694 2 p. |
artikel |
11 |
Fracture toughness of an Al-Li-Cu-In alloy
|
Wagner, John A. |
|
1992 |
26 |
11 |
p. 1779-1784 6 p. |
artikel |
12 |
Improved toughness in Al-Li-Cu-Mg-Ag-Zr alloy X2095
|
Blankenship Jr., C.P. |
|
1992 |
26 |
11 |
p. 1719-1722 4 p. |
artikel |
13 |
Influence of chromium content in a low alloy steel on its tensile properties
|
Chang, Yao-Nan |
|
1992 |
26 |
11 |
p. 1749-1751 3 p. |
artikel |
14 |
Milling maps for phase identification during mechanical alloying
|
Suryanarayana, C. |
|
1992 |
26 |
11 |
p. 1727-1732 6 p. |
artikel |
15 |
Observation of rod-shaped T1 precipitates in an Al-Li-Cu alloy
|
Park, J.K. |
|
1992 |
26 |
11 |
p. 1759-1762 4 p. |
artikel |
16 |
Oxidation kinetics of cast TiAl3
|
Smialek, J.L. |
|
1992 |
26 |
11 |
p. 1763-1768 6 p. |
artikel |
17 |
Phosphorus on the non-brittle grain boundaries of iron
|
Menyhard, M. |
|
1992 |
26 |
11 |
p. 1695-1700 6 p. |
artikel |
18 |
Precipitation in Pb-0.04Ca-1.2Sn alloy
|
Tsubakino, H. |
|
1992 |
26 |
11 |
p. 1681-1685 5 p. |
artikel |
19 |
Redistribution of Ti and Al in deuterium charged TiAl
|
Legzdina, D. |
|
1992 |
26 |
11 |
p. 1737-1741 5 p. |
artikel |
20 |
Reply to: Comments on “Measurement of grain size using the circle intercept method”
|
Willis, D.J. |
|
1992 |
26 |
11 |
p. 1791-1794 4 p. |
artikel |
21 |
Strain induced morphological changes of α 2 and β phases in Ti3Al alloys during superplastic deformation
|
Yang, H.S. |
|
1992 |
26 |
11 |
p. 1707-1712 6 p. |
artikel |
22 |
Structure and properties of Cu, Ni and Fe powders milled in a planetary ball mill
|
Le Brun, P. |
|
1992 |
26 |
11 |
p. 1743-1748 6 p. |
artikel |
23 |
The decrease in yield strength in NiAl due to hydrostatic pressure
|
Margevicius, R.W. |
|
1992 |
26 |
11 |
p. 1733-1736 4 p. |
artikel |
24 |
Thermo-mechanical fatigue of an oxide dispersion strengthened Ni-Cr alloy and its effect on hysteresis loop shape
|
Lindé, L. |
|
1992 |
26 |
11 |
p. 1687-1692 6 p. |
artikel |
25 |
Viscosity limited dislocation motion
|
Kim, C.S. |
|
1992 |
26 |
11 |
p. 1769-1773 5 p. |
artikel |