nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A comparison of viscous flow in sputtered and melt-quenched amorphous Pd/1bSi alloys
|
Volkert, C.A. |
|
1990 |
24 |
3 |
p. 463-467 5 p. |
artikel |
2 |
Amorphization of crystalline CuTi: Roles of chemical disordering and nonequilibrium lattice defects
|
Sabochick, Michael J. |
|
1990 |
24 |
3 |
p. 565-570 6 p. |
artikel |
3 |
A new internal friction peak exceeding the martensitic transformation peak of CuZnAl alloys
|
Harangozò, I.Z. |
|
1990 |
24 |
3 |
p. 475-479 5 p. |
artikel |
4 |
Birefringence observations of dislocation emission at crack tips in NaCl single crystals
|
Foecke, T. |
|
1990 |
24 |
3 |
p. 553-558 6 p. |
artikel |
5 |
Computer simulation of martensitic microstructures
|
Gupta, Rakesh |
|
1990 |
24 |
3 |
p. 533-536 4 p. |
artikel |
6 |
Continuous cooling transformations in Ti3Al + Nb alloys
|
Weykamp, H.T. |
|
1990 |
24 |
3 |
p. 445-450 6 p. |
artikel |
7 |
Effect of beta-phase on serrated yielding in alpha/beta brass
|
Jovanović, M.T. |
|
1990 |
24 |
3 |
p. 547-552 6 p. |
artikel |
8 |
Effect of hydrogen on ultrasonic attenuation in nickel single crystal
|
Zielinski, A. |
|
1990 |
24 |
3 |
p. 521-526 6 p. |
artikel |
9 |
Effects of crain-and grain boundary-strengths on the creep crack growth of HK40 steel
|
Zhu, S.J. |
|
1990 |
24 |
3 |
p. 559-564 6 p. |
artikel |
10 |
Electrochemical permeation of hydrogen in high purity nickel at 100°C
|
Brass, A.M. |
|
1990 |
24 |
3 |
p. 499-504 6 p. |
artikel |
11 |
Extra hardening due to cyclic non-proportional loading of an austenitic stainless steel
|
Doquet, V. |
|
1990 |
24 |
3 |
p. 433-438 6 p. |
artikel |
12 |
Formation and microstructure of localized shear band in a low carbon steel
|
Xu, Y.B. |
|
1990 |
24 |
3 |
p. 571-576 6 p. |
artikel |
13 |
Formation of structural L12 compounds in the ternary Al/1bTi/1bCr system
|
Mabuchi, H. |
|
1990 |
24 |
3 |
p. 505-508 4 p. |
artikel |
14 |
Influence of minor additions of Zr on the mechanical behaviour of a Mg/1bLi/1bAl alloy
|
Singh, R.K. |
|
1990 |
24 |
3 |
p. 451-456 6 p. |
artikel |
15 |
Interfacial properties measurement for SiC fiber-reinforced titantum alloy composites
|
Yang, C.J. |
|
1990 |
24 |
3 |
p. 469-474 6 p. |
artikel |
16 |
Lattice parameters of iron-carbon and iron-nitrogen martensites and austenites
|
Cheng, Liu |
|
1990 |
24 |
3 |
p. 509-514 6 p. |
artikel |
17 |
Liquid film migration (LFM) in the weld heat affected zone (HAZ) of a ni-base superalloy
|
Radhakrishnan, B. |
|
1990 |
24 |
3 |
p. 537-542 6 p. |
artikel |
18 |
Nucleation and growth of cavities at defined grain boundaries in bicrystals
|
Lombard, R. |
|
1990 |
24 |
3 |
p. 581-586 6 p. |
artikel |
19 |
Orientational dependence of the temperature of ductile-to-brittle transition of molybdenum single crystals
|
Dobromyslov, A.V. |
|
1990 |
24 |
3 |
p. 543-546 4 p. |
artikel |
20 |
Orientation relationship of the needle-like phase in a duplex Fe/1bMn/1bAl/1bC alloy
|
Hwang, K.H. |
|
1990 |
24 |
3 |
p. 495-498 4 p. |
artikel |
21 |
Positive temperature dependence of the yield stress in L1o type Ti/1bAl/1bV compound
|
Whang, S.H. |
|
1990 |
24 |
3 |
p. 485-490 6 p. |
artikel |
22 |
Preparation and consolidation of Al-based alloy quasicrystalline powders
|
Zhenhua, Chen |
|
1990 |
24 |
3 |
p. 599-603 5 p. |
artikel |
23 |
Secondary hardening embrittlement in the peak-aged 6W-6Ni steel
|
Kim, Kwang-Hoon |
|
1990 |
24 |
3 |
p. 515-520 6 p. |
artikel |
24 |
Solidification structures during laser treatment
|
Hegge, H.J. |
|
1990 |
24 |
3 |
p. 593-598 6 p. |
artikel |
25 |
Some results on the phase behavior in coherent equilibria
|
Larché, Francis C. |
|
1990 |
24 |
3 |
p. 491-493 3 p. |
artikel |
26 |
Spall failure in 6061/SiC particulate metal matrix composite
|
Dixon, D.G. |
|
1990 |
24 |
3 |
p. 577-580 4 p. |
artikel |
27 |
The constitution of alloys of germanium with the compound AuGa2
|
Butt, M.T.Z. |
|
1990 |
24 |
3 |
p. 481-484 4 p. |
artikel |
28 |
The determination of degree of order of nearby grain boundary in the Ni3A1 family
|
Zhu, Jing |
|
1990 |
24 |
3 |
p. 439-443 5 p. |
artikel |
29 |
Time-dependent failure of silver-interlayer diffusion welds between elastically-deforming base metals
|
Kassner, M.E. |
|
1990 |
24 |
3 |
p. 587-592 6 p. |
artikel |
30 |
Ultra-high-strength, forgeable Al/1bCu/1bLi/1bAg/1bMg alloy
|
Pickens, J.R. |
|
1990 |
24 |
3 |
p. 457-462 6 p. |
artikel |
31 |
Ultrasonic attenuation in hydrogen charged copper single crystal
|
Zielinski, A. |
|
1990 |
24 |
3 |
p. 527-532 6 p. |
artikel |