nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Amorphisation compositional limits and atomic displacement in fcc solid solutions
|
Delogu, F. |
|
2004 |
383 |
2 |
p. 252-258 7 p. |
artikel |
2 |
An investigation of the embrittlement in X20CrMoV12.1 power plant steel after long-term service exposure at elevated temperature
|
Hu, Zheng-Fei |
|
2004 |
383 |
2 |
p. 224-228 5 p. |
artikel |
3 |
Apparent viscosity of W–Cu powder compacts during sintering
|
Doré, F. |
|
2004 |
383 |
2 |
p. 390-398 9 p. |
artikel |
4 |
Author Index
|
|
|
2004 |
383 |
2 |
p. 399-400 2 p. |
artikel |
5 |
Carbonate Co-precipitation of Gd2O3-doped CeO2 solid solution nano-particles
|
Tok, A.I.Y. |
|
2004 |
383 |
2 |
p. 229-234 6 p. |
artikel |
6 |
Characterization of tensile damage and strength in GFRP cross-ply laminates
|
Okabe, T. |
|
2004 |
383 |
2 |
p. 381-389 9 p. |
artikel |
7 |
Constitutive behaviour of A356 during the quenching operation
|
Estey, C.M. |
|
2004 |
383 |
2 |
p. 245-251 7 p. |
artikel |
8 |
Correlation between the mechanical properties and the microstructural behaviour of Al2O3–(Ag–Cu–Ti) brazed joints
|
Mandal, Sudipta |
|
2004 |
383 |
2 |
p. 235-244 10 p. |
artikel |
9 |
Direct laser sintering of iron–graphite powder mixture
|
Simchi, A. |
|
2004 |
383 |
2 |
p. 191-200 10 p. |
artikel |
10 |
Effect of rare earth element on microstructure formation and mechanical properties of thin wall ductile iron castings
|
Choi, J.O. |
|
2004 |
383 |
2 |
p. 323-333 11 p. |
artikel |
11 |
Effect of surface treatments on fatigue life of Ti-6-22-22 alloy at room and high temperatures
|
Yu, Z.L. |
|
2004 |
383 |
2 |
p. 283-288 6 p. |
artikel |
12 |
Effect of thermomechanical working on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718
|
Appa Rao, G. |
|
2004 |
383 |
2 |
p. 201-212 12 p. |
artikel |
13 |
Effects of microstructure on fretting fatigue crack initiation behavior of Ti-6Al-4V
|
Mall, S. |
|
2004 |
383 |
2 |
p. 334-340 7 p. |
artikel |
14 |
Influence of melt convection on dendritic spacings of downward unsteady-state directionally solidified Al–Cu alloys
|
Spinelli, José E. |
|
2004 |
383 |
2 |
p. 271-282 12 p. |
artikel |
15 |
Inside Front Cover: Editorial Board
|
|
|
2004 |
383 |
2 |
p. IFC- 1 p. |
artikel |
16 |
In situ observation of fracture behavior of in situ TiBw/Ti composites
|
Li, B.S. |
|
2004 |
383 |
2 |
p. 316-322 7 p. |
artikel |
17 |
Microstructure, tensile strength and wear behaviour of Al–Sc alloy
|
Venkateswarlu, K. |
|
2004 |
383 |
2 |
p. 374-380 7 p. |
artikel |
18 |
Miscibility, structure and properties of PP/PIB blends
|
Szabó, Péter |
|
2004 |
383 |
2 |
p. 307-315 9 p. |
artikel |
19 |
Modeling the influence of the nature of spatial heterogeneity on the deformation and failure of porous ductile alloys
|
Khvastunkov, Mikhail S. |
|
2004 |
383 |
2 |
p. 347-355 9 p. |
artikel |
20 |
Optimization of thermal treatment parameters to alter austenitic phase transition temperature of NiTi alloy for medical implant
|
Yeung, K.W.K. |
|
2004 |
383 |
2 |
p. 213-218 6 p. |
artikel |
21 |
Pure Al matrix composites produced by vacuum hot pressing: tensile properties and strengthening mechanisms
|
Tang, Fei |
|
2004 |
383 |
2 |
p. 362-373 12 p. |
artikel |
22 |
Shear band formation and ductility of metallic glasses
|
Sergueeva, A.V. |
|
2004 |
383 |
2 |
p. 219-223 5 p. |
artikel |
23 |
Shear features during equal channel angular pressing of a lamellae eutectic alloy
|
Wang, Jingtao |
|
2004 |
383 |
2 |
p. 356-361 6 p. |
artikel |
24 |
Subject Index
|
|
|
2004 |
383 |
2 |
p. 401-405 5 p. |
artikel |
25 |
Surface modification of 2014 aluminium alloy–Al2O3 particles composites by nickel electrochemical deposition
|
Molina, J.M. |
|
2004 |
383 |
2 |
p. 299-306 8 p. |
artikel |
26 |
The annealing and aging effects of high temperature internal friction in pure aluminum
|
Cao, Xiaohui |
|
2004 |
383 |
2 |
p. 341-346 6 p. |
artikel |
27 |
The effect of iron and manganese on the formation of intermetallic compounds in aluminum–silicon alloys
|
Shabestari, S.G. |
|
2004 |
383 |
2 |
p. 289-298 10 p. |
artikel |
28 |
The effect of second-phase Ni solid solution on environmental embrittlement of L12-type Ni3(Si,Ti) ordered alloys
|
Nakamura, T. |
|
2004 |
383 |
2 |
p. 259-270 12 p. |
artikel |