nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A comparative investigation of the friction and wear behavior of polyimide composites under dry sliding and water-lubricated condition
|
Jia, J.H |
|
2003 |
356 |
1-2 |
p. 48-53 6 p. |
artikel |
2 |
Ageing of martensite: stabilisation and ferroelasticity in Cu-based shape memory alloys
|
Ahlers, M. |
|
2003 |
356 |
1-2 |
p. 298-315 18 p. |
artikel |
3 |
Al2O3/Ti(C0.3N0.7) cutting tool material
|
Song, Shi-Xue |
|
2003 |
356 |
1-2 |
p. 43-47 5 p. |
artikel |
4 |
A physically based model for TRIP-aided carbon steels behaviour
|
Perlade, A. |
|
2003 |
356 |
1-2 |
p. 145-152 8 p. |
artikel |
5 |
Author Index
|
|
|
2003 |
356 |
1-2 |
p. 464-465 2 p. |
artikel |
6 |
Characterization and mechanical properties of in situ synthesized Ti5Si3/TiAl composites
|
Rao, K.P. |
|
2003 |
356 |
1-2 |
p. 208-218 11 p. |
artikel |
7 |
Chronological study of the oxidation of phosphated α-iron
|
Panicaud, B |
|
2003 |
356 |
1-2 |
p. 434-442 9 p. |
artikel |
8 |
Codeposition of Al and Si on nickel base superalloys by pack cementation process
|
Xiang, Z.D. |
|
2003 |
356 |
1-2 |
p. 136-144 9 p. |
artikel |
9 |
Cyclic deformation and fatigue crack propagation of a Zr-based bulk amorphous metal
|
Zhang, H. |
|
2003 |
356 |
1-2 |
p. 173-180 8 p. |
artikel |
10 |
Dehydrogenation of TiH2
|
Bhosle, V |
|
2003 |
356 |
1-2 |
p. 190-199 10 p. |
artikel |
11 |
Dissolution kinetics of delta ferrite in AISI 304 stainless steel produced by strip casting process
|
Kim, S.H. |
|
2003 |
356 |
1-2 |
p. 390-398 9 p. |
artikel |
12 |
Effect of an electric field on microstructure coarsening in 60Sn40Pb solder joints
|
Jung, Kang |
|
2003 |
356 |
1-2 |
p. 8-16 9 p. |
artikel |
13 |
Effect of dual torch technique on duplex stainless steel welds
|
Sun, Z. |
|
2003 |
356 |
1-2 |
p. 274-282 9 p. |
artikel |
14 |
Effect of mixing on the rheology and particle characteristics of tungsten-based powder injection molding feedstock
|
Suri, Pavan |
|
2003 |
356 |
1-2 |
p. 337-344 8 p. |
artikel |
15 |
Effect of spark plasma sintering (SPS) on the microstructure and mechanical properties of randomly packed hollow sphere (RHS) cell wall
|
Khor, K.A. |
|
2003 |
356 |
1-2 |
p. 130-135 6 p. |
artikel |
16 |
Effects of loading frequency on fatigue crack growth mechanisms in α/β Ti microstructure with large colony size
|
Sansoz, F. |
|
2003 |
356 |
1-2 |
p. 81-92 12 p. |
artikel |
17 |
Effects of thermal residual stress creeping on microstructure and tensile properties of SiC whisker reinforced aluminum matrix composite
|
Fei, W.D. |
|
2003 |
356 |
1-2 |
p. 17-22 6 p. |
artikel |
18 |
Effects of tooling on the residual stress distribution in an inertia weld
|
Pang, J.W.L |
|
2003 |
356 |
1-2 |
p. 405-413 9 p. |
artikel |
19 |
Experimental investigation of the transient and steady state rheological behaviour of Al–Si alloys in the mushy state
|
Brabazon, D |
|
2003 |
356 |
1-2 |
p. 69-80 12 p. |
artikel |
20 |
Fabrication of NiTi intermetallic compound by a reactive gas laser atomization process
|
Tomochika, Hiroshi |
|
2003 |
356 |
1-2 |
p. 122-129 8 p. |
artikel |
21 |
Fatigue crack growth behavior of off-axis Ti–6Al–4V/SCS-6 metal matrix composites
|
Yasmin, A |
|
2003 |
356 |
1-2 |
p. 54-68 15 p. |
artikel |
22 |
Fatigue crack growth in polycrystalline IN 718 superalloy
|
Osinkolu, G.A |
|
2003 |
356 |
1-2 |
p. 425-433 9 p. |
artikel |
23 |
Fatigue crack propagation normal to a plasticity mismatched bimaterial interface
|
Jiang, F. |
|
2003 |
356 |
1-2 |
p. 258-266 9 p. |
artikel |
24 |
Flow stress and microstructure of the cold-rolled IF-steel
|
Li, B.L. |
|
2003 |
356 |
1-2 |
p. 37-42 6 p. |
artikel |
25 |
Identification of the principal elements governing the wettability characteristics of ordinary Portland cement following high power diode laser surface treatment
|
Lawrence, J |
|
2003 |
356 |
1-2 |
p. 162-172 11 p. |
artikel |
26 |
Influence of the content of ceramic phase on the precipitation hardening of Al alloy 7000/AlN nanocomposites
|
Goujon, C |
|
2003 |
356 |
1-2 |
p. 399-404 6 p. |
artikel |
27 |
Mechanical properties of modified 9Cr–1Mo steel welds with notches
|
Lee, W.H. |
|
2003 |
356 |
1-2 |
p. 153-161 9 p. |
artikel |
28 |
Mechanism of 〈112〉/3 slip initiation and anisotropy of γ′ phase in CMSX-4 during creep at 750°C and 750 MPa
|
Chen, Q.Z. |
|
2003 |
356 |
1-2 |
p. 352-367 16 p. |
artikel |
29 |
Mechanisms of microstructure evolution during cryomilling in the presence of hard particles
|
Chung, Kyung H |
|
2003 |
356 |
1-2 |
p. 23-31 9 p. |
artikel |
30 |
Melt ejection during laser drilling of metals
|
Voisey, K.T. |
|
2003 |
356 |
1-2 |
p. 414-424 11 p. |
artikel |
31 |
Microstructure and mechanical properties of Mg–Al based alloy with calcium and rare earth additions
|
Wenwen, Du |
|
2003 |
356 |
1-2 |
p. 1-7 7 p. |
artikel |
32 |
Microstructure and some magnetic properties of annealed Vitrovac® 6025X amorphous ribbons
|
Świerczek, J. |
|
2003 |
356 |
1-2 |
p. 108-113 6 p. |
artikel |
33 |
Microstructure and thermoelectric properties of extruded n-type 95%Bi2Te2–5%Bi2Se3 alloy along bar length
|
Hong, Soon-Jik |
|
2003 |
356 |
1-2 |
p. 345-351 7 p. |
artikel |
34 |
Microstructures of binderless tungsten carbides sintered by spark plasma sintering process
|
Cha, Seung I. |
|
2003 |
356 |
1-2 |
p. 381-389 9 p. |
artikel |
35 |
Microwave sintering of MoSi2–SiC composites
|
Panneerselvam, M. |
|
2003 |
356 |
1-2 |
p. 267-273 7 p. |
artikel |
36 |
On the experimental characterization of crystal plasticity in polycrystals
|
Tatschl, A. |
|
2003 |
356 |
1-2 |
p. 447-463 17 p. |
artikel |
37 |
On the relationship between microstructure, strength and toughness in AA7050 aluminum alloy
|
Dumont, D. |
|
2003 |
356 |
1-2 |
p. 326-336 11 p. |
artikel |
38 |
Precipitation in a Cu–Cr–Zr alloy
|
Batra, I.S. |
|
2003 |
356 |
1-2 |
p. 32-36 5 p. |
artikel |
39 |
Production of nanocrystalline cermet thermal spray powders for wear resistant coatings by high-energy milling
|
Eigen, N |
|
2003 |
356 |
1-2 |
p. 114-121 8 p. |
artikel |
40 |
Protection of titanium alloy components against high temperature corrosion
|
Gurappa, I. |
|
2003 |
356 |
1-2 |
p. 372-380 9 p. |
artikel |
41 |
Role of strain path change in texture development
|
Suwas, Satyam |
|
2003 |
356 |
1-2 |
p. 368-371 4 p. |
artikel |
42 |
Spark-plasma-sintered BaTiO3/Al2O3 nanocomposites
|
Zhan, Guo-Dong |
|
2003 |
356 |
1-2 |
p. 443-446 4 p. |
artikel |
43 |
Spatial pattern analysis of second-phase particles in composite materials
|
Scalon, J.D. |
|
2003 |
356 |
1-2 |
p. 245-257 13 p. |
artikel |
44 |
Studies on mechanical interfacial properties of oxy-fluorinated carbon fibers-reinforced composites
|
Park, Soo-Jin |
|
2003 |
356 |
1-2 |
p. 219-226 8 p. |
artikel |
45 |
Subject Index
|
|
|
2003 |
356 |
1-2 |
p. 466-471 6 p. |
artikel |
46 |
Tensile creep of polycrystalline near-stoichiometric NiAl
|
Raj, S.V. |
|
2003 |
356 |
1-2 |
p. 283-297 15 p. |
artikel |
47 |
The emission of dislocations from crack tips
|
Schoeck, Gunther |
|
2003 |
356 |
1-2 |
p. 93-101 9 p. |
artikel |
48 |
Thermal treatment of PM-tool steel alloyed with niobium
|
Pavlı́čková, M. |
|
2003 |
356 |
1-2 |
p. 200-207 8 p. |
artikel |
49 |
The thermal stability of TiC particles in an Al7wt.%Si alloy
|
López, V.H. |
|
2003 |
356 |
1-2 |
p. 316-325 10 p. |
artikel |
50 |
Time distribution of stress drops, critical strain and crossover in the dynamics of jerky flow
|
Chihab, K. |
|
2003 |
356 |
1-2 |
p. 102-107 6 p. |
artikel |
51 |
Ultra-long cycle fatigue of high-strength carbon steels part II: estimation of fatigue limit for failure from internal inclusions
|
Chapetti, M.D. |
|
2003 |
356 |
1-2 |
p. 236-244 9 p. |
artikel |
52 |
Ultra-long cycle fatigue of high-strength carbon steels part I: review and analysis of the mechanism of failure
|
Chapetti, M.D. |
|
2003 |
356 |
1-2 |
p. 227-235 9 p. |
artikel |
53 |
Vapour phase codeposition of Al and Si to form diffusion coatings on γ-TiAl
|
Xiang, Z.D. |
|
2003 |
356 |
1-2 |
p. 181-189 9 p. |
artikel |