nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Activation energy calculations for discontinuous yielding in Inconel 718SPF
|
Hale, C.L |
|
2001 |
300 |
1-2 |
p. 153-164 12 p. |
artikel |
2 |
Aluminium nitride by plasma spraying of an Al2O3–C–Sm2O3 system
|
Khor, K.A |
|
2001 |
300 |
1-2 |
p. 203-210 8 p. |
artikel |
3 |
Analysis of misorientation distribution in polycrystalline aluminum sheet by using ODF data
|
Mao, Weimin |
|
2001 |
300 |
1-2 |
p. 80-84 5 p. |
artikel |
4 |
An experimental study on deformation behavior below 0.2% offset yield stress in some SiCp/Al composites and their unreinforced matrix alloys
|
Zhang, Fan |
|
2001 |
300 |
1-2 |
p. 12-21 10 p. |
artikel |
5 |
Combined effect of special grain boundaries and grain boundary carbides on IGSCC of Ni–16Cr–9Fe–xC alloys
|
Alexandreanu, Bogdan |
|
2001 |
300 |
1-2 |
p. 94-104 11 p. |
artikel |
6 |
Creep of magnesium strengthened with high volume fractions of yttria dispersoids
|
Han, B.Q |
|
2001 |
300 |
1-2 |
p. 235-244 10 p. |
artikel |
7 |
Determination of steep stress gradients by X-ray diffraction — results of a joint investigation
|
Behnken, H. |
|
2001 |
300 |
1-2 |
p. 41-51 11 p. |
artikel |
8 |
Development of a modified CVD coating process for the enhancement of the high temperature oxidation resistance of Cr2O3 and Al2O3 forming alloys
|
Paúl, A |
|
2001 |
300 |
1-2 |
p. 22-33 12 p. |
artikel |
9 |
Development of SiC/TiAl composites: processing and interfacial phenomena
|
Djanarthany, Sarala |
|
2001 |
300 |
1-2 |
p. 211-218 8 p. |
artikel |
10 |
Discussion on ‘influence of applied electric field and mechanical boundary condition on the stress distribution at the crack tip in piezoelectric materials 1 Kumar S, Singh RN, (1997), Influence of applied electric field and mechanical boundary condition on the stress distribution at the crack tip in piezoelectric materials, Materials Science and Engineering A231 pp 1–9. 1 ’
|
Tian-hu, Hao |
|
2001 |
300 |
1-2 |
p. 316-318 3 p. |
artikel |
11 |
Dislocation structures in cyclically deformed nickel polycrystals
|
Buque, C |
|
2001 |
300 |
1-2 |
p. 254-262 9 p. |
artikel |
12 |
Effect of carbon interlayer on oxidation behavior of C/SiC composites with a coating from room temperature to 1500°C
|
Cheng, Laifei |
|
2001 |
300 |
1-2 |
p. 219-225 7 p. |
artikel |
13 |
Effect of heating rate on the grain refinement of a TiAl alloy by cyclic heat treatment
|
Xia, Qiangfei |
|
2001 |
300 |
1-2 |
p. 309-311 3 p. |
artikel |
14 |
Fabrication and mechanical properties of steel–steel composites
|
Sun, Shoujin |
|
2001 |
300 |
1-2 |
p. 135-141 7 p. |
artikel |
15 |
Fracture toughness of intermetallic compacts consolidated from nanocrystalline powders
|
Varin, R.A |
|
2001 |
300 |
1-2 |
p. 1-11 11 p. |
artikel |
16 |
Heat and mass transfer during in-flight nitridation of molybdenum disilicide powder in an induction plasma reactor
|
Soucy, Gervais |
|
2001 |
300 |
1-2 |
p. 226-234 9 p. |
artikel |
17 |
High-temperature creep of a bi-directional, continuous-SiC-fiber-reinforced glass-ceramic composite
|
Nair, B.G |
|
2001 |
300 |
1-2 |
p. 68-79 12 p. |
artikel |
18 |
High temperature creep of a hot-pressed β-sialon
|
Lin, M.T. |
|
2001 |
300 |
1-2 |
p. 61-67 7 p. |
artikel |
19 |
Hot corrosion of atomized iron aluminides doped with boron and reinforced with alumina
|
Espinosa-Medina, M.A. |
|
2001 |
300 |
1-2 |
p. 183-189 7 p. |
artikel |
20 |
HREM observations of the synthesized process of nano-sized SiC by ball milling of Si and C mixed powders
|
Yang, X.Y. |
|
2001 |
300 |
1-2 |
p. 278-283 6 p. |
artikel |
21 |
Hydrogen-enhanced microplasticity of austenitic steels studied by means of internal friction
|
Shivanyuk, V.N |
|
2001 |
300 |
1-2 |
p. 284-290 7 p. |
artikel |
22 |
Hydrogen evolution on hot and cold consolidated Ni–Mo alloys produced by mechanical alloying
|
Kedzierzawski, P |
|
2001 |
300 |
1-2 |
p. 105-112 8 p. |
artikel |
23 |
(Icosahedral phase+α-Mg) two phase microstructures in the Mg–Zn–Y ternary system
|
Yi, S. |
|
2001 |
300 |
1-2 |
p. 312-315 4 p. |
artikel |
24 |
Improving the mechanical properties of magnesium and a magnesium alloy through severe plastic deformation
|
Yamashita, Akihiro |
|
2001 |
300 |
1-2 |
p. 142-147 6 p. |
artikel |
25 |
Index
|
|
|
2001 |
300 |
1-2 |
p. 319- 1 p. |
artikel |
26 |
Index
|
|
|
2001 |
300 |
1-2 |
p. 320-323 4 p. |
artikel |
27 |
Low-temperature superplasticity of titanium aluminides
|
Imayev, R.M |
|
2001 |
300 |
1-2 |
p. 263-277 15 p. |
artikel |
28 |
Mechanical properties of 3D fiber reinforced C/SiC composites
|
Xu, Yongdong |
|
2001 |
300 |
1-2 |
p. 196-202 7 p. |
artikel |
29 |
Microstructural characterisation of defect structures in a TiAl-base Ti–47Al–2Nb–2Mn(at.%)+0.8vol.%TiB2 alloy
|
Chen, S.H |
|
2001 |
300 |
1-2 |
p. 299-308 10 p. |
artikel |
30 |
Numerical modelling of particle distribution effects on fatigue in Al–SiCp composites
|
Boselli, J |
|
2001 |
300 |
1-2 |
p. 113-124 12 p. |
artikel |
31 |
Overview of fatigue properties of fine grain 5056 Al-Mg alloy processed by equal-channel angular pressing
|
Patlan, V. |
|
2001 |
300 |
1-2 |
p. 171-182 12 p. |
artikel |
32 |
Solution heat treatment response of a third generation single crystal Ni-base superalloy
|
Fuchs, G.E. |
|
2001 |
300 |
1-2 |
p. 52-60 9 p. |
artikel |
33 |
Special shell mold for solidification of undercooled nickel-based alloy melts
|
Feng, Liu |
|
2001 |
300 |
1-2 |
p. 190-195 6 p. |
artikel |
34 |
Strain–anneal growth of Zr 701 large crystals
|
Chaubet, D |
|
2001 |
300 |
1-2 |
p. 245-253 9 p. |
artikel |
35 |
Strain localisation in solution heat treated Al–Zn–Mg alloys
|
Fjeldly, Alexander |
|
2001 |
300 |
1-2 |
p. 165-170 6 p. |
artikel |
36 |
Structural evolution of the Ti70Ni15Al15 powders prepared by mechanical alloying
|
Kim, K.B. |
|
2001 |
300 |
1-2 |
p. 148-152 5 p. |
artikel |
37 |
Synthesis and characterization of a TiAl/Ti5Si3 composite with a submicrocrystalline structure
|
Senkov, O.N |
|
2001 |
300 |
1-2 |
p. 85-93 9 p. |
artikel |
38 |
The oxygen-wetting transition in metal/oxide systems
|
Eustathopoulos, N |
|
2001 |
300 |
1-2 |
p. 34-40 7 p. |
artikel |
39 |
The role of stacking fault shear in the primary creep of [001]-oriented single crystal superalloys at 750°C and 750 MPa
|
Rae, C.M.F. |
|
2001 |
300 |
1-2 |
p. 125-134 10 p. |
artikel |
40 |
Two way shape memory loss in CuZnAl alloy
|
Datta, S |
|
2001 |
300 |
1-2 |
p. 291-298 8 p. |
artikel |