nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
An analysis of electrical resistivity of compositions within the Mo–Si–B ternary system part II: Multi-phase composites
|
Beckman, S |
|
2001 |
299 |
1-2 |
p. 94-104 11 p. |
artikel |
2 |
Anisotropic mechanical properties of porous copper fabricated by unidirectional solidification
|
Hyun, S.K |
|
2001 |
299 |
1-2 |
p. 241-248 8 p. |
artikel |
3 |
Anisotropy and strain localization in steel foam
|
Park, C |
|
2001 |
299 |
1-2 |
p. 68-74 7 p. |
artikel |
4 |
Characterization and performance of laser melted AZ91D and AM60B
|
Dubé, D. |
|
2001 |
299 |
1-2 |
p. 38-45 8 p. |
artikel |
5 |
Comparison of keyhole and conventional gas tungsten arc welds in commercially pure titanium
|
Lathabai, S. |
|
2001 |
299 |
1-2 |
p. 81-93 13 p. |
artikel |
6 |
Consolidation behavior of SiC powder under cold compaction
|
Park, H. |
|
2001 |
299 |
1-2 |
p. 116-124 9 p. |
artikel |
7 |
Fatigue crack propagation in 2.25 Cr–1.0Mo steel weldments in air and hydrogen
|
Tsay, L.W. |
|
2001 |
299 |
1-2 |
p. 16-26 11 p. |
artikel |
8 |
Finite element analysis of torsional deformation
|
Kim, Hyoung Seop |
|
2001 |
299 |
1-2 |
p. 305-308 4 p. |
artikel |
9 |
Grain morphology of molybdenum splats plasma-sprayed on glass substrates
|
Jiang, Xiangyang |
|
2001 |
299 |
1-2 |
p. 235-240 6 p. |
artikel |
10 |
Index
|
|
|
2001 |
299 |
1-2 |
p. 309- 1 p. |
artikel |
11 |
Index
|
|
|
2001 |
299 |
1-2 |
p. 310-313 4 p. |
artikel |
12 |
Influence of ECAP routes on the microstructure and properties of pure Ti
|
Stolyarov, Vladimir V |
|
2001 |
299 |
1-2 |
p. 59-67 9 p. |
artikel |
13 |
Influence of temperature and strain rate on the flow stress of an FeAl alloy
|
Sastry, D.H |
|
2001 |
299 |
1-2 |
p. 157-163 7 p. |
artikel |
14 |
Influence on texture on beta grain growth during continuous annealing of Ti–6Al–4V
|
Semiatin, S.L |
|
2001 |
299 |
1-2 |
p. 225-234 10 p. |
artikel |
15 |
Microstructural changes due to heat-treatment of annealing and their effect on the creep behavior of self-reinforced silicon nitride ceramics
|
Wei, Q |
|
2001 |
299 |
1-2 |
p. 141-151 11 p. |
artikel |
16 |
Microstructural factors of low cycle fatigue damage in two phase Al–Si alloys
|
Stolarz, Jacques |
|
2001 |
299 |
1-2 |
p. 275-286 12 p. |
artikel |
17 |
Microstructure controlling by heat treatment and complex processing for Ti2AlNb based alloys
|
Peng, Jihua |
|
2001 |
299 |
1-2 |
p. 75-80 6 p. |
artikel |
18 |
Microstructures and tensile properties of Ti–45.5Al–2Nb–2Cr rolled sheets
|
Seetharaman, V |
|
2001 |
299 |
1-2 |
p. 195-209 15 p. |
artikel |
19 |
Physico-chemical analyses and solidification path reconstruction of multi-component oxidic spread melts
|
Journeau, C |
|
2001 |
299 |
1-2 |
p. 249-266 18 p. |
artikel |
20 |
Rapid prototyping and combustion synthesis of TiC/Ni functionally gradient materials
|
Zhang, Yumin |
|
2001 |
299 |
1-2 |
p. 218-224 7 p. |
artikel |
21 |
Review: reaction synthesis processing of Ni–Al intermetallic materials
|
Morsi, K. |
|
2001 |
299 |
1-2 |
p. 1-15 15 p. |
artikel |
22 |
Room temperature mechanical behavior of B2-ordered Fe3Al single crystals
|
Zheng, W.W. |
|
2001 |
299 |
1-2 |
p. 46-50 5 p. |
artikel |
23 |
Semi-solid processing of engineering alloys by a twin-screw rheomoulding process
|
Ji, S |
|
2001 |
299 |
1-2 |
p. 210-217 8 p. |
artikel |
24 |
Shear localization and recrystallization in dynamic deformation of 8090 Al–Li alloy
|
Xu, Y.B. |
|
2001 |
299 |
1-2 |
p. 287-295 9 p. |
artikel |
25 |
Simulation and observation of dislocation pattern evolution in the early stages of fatigue in a copper single crystal
|
Yang, Jihong |
|
2001 |
299 |
1-2 |
p. 51-58 8 p. |
artikel |
26 |
Stability of the bulk glass-forming Mg65Y10Cu25 alloy in aqueous electrolytes
|
Gebert, A |
|
2001 |
299 |
1-2 |
p. 125-135 11 p. |
artikel |
27 |
Strain-induced precipitation behaviour in hot rolled strip steel
|
Pereloma, E.V |
|
2001 |
299 |
1-2 |
p. 27-37 11 p. |
artikel |
28 |
Substructures of deformation twins and twin intersections in a Ti–45Al–8Nb–2.5Mn alloy heavily deformed at room temperature
|
Zhang, L.C. |
|
2001 |
299 |
1-2 |
p. 267-274 8 p. |
artikel |
29 |
Superhard carbon particles forming from fullerites in a mixture with iron powder
|
Tchernogorova, O.P |
|
2001 |
299 |
1-2 |
p. 136-140 5 p. |
artikel |
30 |
Synthesis and properties of cubic zirconia–alumina composite by mechanical alloying
|
Kwon, Nam-Hee |
|
2001 |
299 |
1-2 |
p. 185-194 10 p. |
artikel |
31 |
The effect of β, β′ and β″ precipitates in a homogenised AA6063 alloy on the hot deformability and the peak hardness
|
van de Langkruis, J |
|
2001 |
299 |
1-2 |
p. 105-115 11 p. |
artikel |
32 |
The high-temperature performance of nickel-based transition joints
|
Parker, J.D |
|
2001 |
299 |
1-2 |
p. 164-173 10 p. |
artikel |
33 |
The high-temperature performance of nickel-based transition joints
|
Parker, J.D |
|
2001 |
299 |
1-2 |
p. 174-184 11 p. |
artikel |
34 |
Thermal fatigue of single-crystalline superalloy CMSX-4®: a comparison of epitaxial laser-deposited material with the base single crystal
|
Felberbaum, L |
|
2001 |
299 |
1-2 |
p. 152-156 5 p. |
artikel |
35 |
Thermal fracture of ceramic thermal barrier coatings under high heat flux with time-dependent behavior.
|
Choules, Brian D |
|
2001 |
299 |
1-2 |
p. 296-304 9 p. |
artikel |