nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Activation processes of stress relaxation during hold time in 1Cr–Mo–V steel
|
Jeong, Chang Yeol |
|
1999 |
264 |
1-2 |
p. 188-193 6 p. |
artikel |
2 |
Analysis and prevention of edge cracking phenomenon during hot rolling of non-oriented electrical steel sheets
|
Han, Myung Hwan |
|
1999 |
264 |
1-2 |
p. 47-59 13 p. |
artikel |
3 |
Analysis of small-angle neutron scattering from Fe–18Cr–10Mn–16Ni–0.5N and Fe–21Cr–10Mn–17Ni–0.5C austenites
|
Nadutov, V.M. |
|
1999 |
264 |
1-2 |
p. 286-290 5 p. |
artikel |
4 |
An investigation of fracture and fatigue crack growth behavior of cast niobium aluminide intermetallics
|
Ye, F |
|
1999 |
264 |
1-2 |
p. 81-93 13 p. |
artikel |
5 |
Ball indentation studies on the effect of aging on mechanical behavior of alloy 625
|
Mathew, M.D |
|
1999 |
264 |
1-2 |
p. 159-166 8 p. |
artikel |
6 |
Cyclic and static creep behavior of Al–Cu alloy composite reinforced with in-situ Al2O3 and TiB2 particulates
|
Ma, Z.Y |
|
1999 |
264 |
1-2 |
p. 177-187 11 p. |
artikel |
7 |
Cyclic deformation and near surface microstructures of shot peened or deep rolled austenitic stainless steel AISI 304
|
Altenberger, I |
|
1999 |
264 |
1-2 |
p. 1-16 16 p. |
artikel |
8 |
Cyclic stress–strain response of superelastic Cu–Al–Mn alloy single crystals
|
Kato, Hiroyuki |
|
1999 |
264 |
1-2 |
p. 245-253 9 p. |
artikel |
9 |
Densification of sintered molybdenum during hot upsetting: experiments and modelling
|
Parteder, E. |
|
1999 |
264 |
1-2 |
p. 17-25 9 p. |
artikel |
10 |
Determination of the precipitation kinetics of Ni3Al in the Ni–Al system using differential scanning calorimetry
|
Jackson, M.P. |
|
1999 |
264 |
1-2 |
p. 26-38 13 p. |
artikel |
11 |
Effect of f.c.c. antiferromagnetism on martensitic transformation in Fe–Mn–Si based alloys
|
Chen, Shuchuan |
|
1999 |
264 |
1-2 |
p. 262-268 7 p. |
artikel |
12 |
Effect of niobium filaments on mechanical response and fracture characteristics of dispersion strengthened copper alloy and copper–niobium microcomposite
|
Srivatsan, T.S |
|
1999 |
264 |
1-2 |
p. 60-73 14 p. |
artikel |
13 |
Effects of buoyancy convection on phase morphology during solidification of Pd40Ni40P20 alloy
|
Liu, R.P. |
|
1999 |
264 |
1-2 |
p. 167-171 5 p. |
artikel |
14 |
Enhancement of self-sustaining reaction by mechanical activation: case of an FeSi system
|
Gras, C |
|
1999 |
264 |
1-2 |
p. 94-107 14 p. |
artikel |
15 |
Fatigue fracture at copper bicrystal interfaces: fractography
|
Peralta, P |
|
1999 |
264 |
1-2 |
p. 215-231 17 p. |
artikel |
16 |
High-temperature corrosion of Fe3Al in chlorine-containing environments
|
Kim, I. |
|
1999 |
264 |
1-2 |
p. 269-278 10 p. |
artikel |
17 |
Index
|
|
|
1999 |
264 |
1-2 |
p. 291- 1 p. |
artikel |
18 |
Index
|
|
|
1999 |
264 |
1-2 |
p. 292-295 4 p. |
artikel |
19 |
Influence of process variables on press bonding of superplastic 8090 Al–Li alloy
|
Wu, Horng-yu |
|
1999 |
264 |
1-2 |
p. 194-200 7 p. |
artikel |
20 |
Influence of trace elements and heat treatment on carbide morphology and properties of CD-2 steel
|
Wang, S.Q. |
|
1999 |
264 |
1-2 |
p. 172-176 5 p. |
artikel |
21 |
Kinetics of the phase transformation and wear resistance of in-situ processed titanium matrix composites based on Ti–Fe–B
|
Bram, M. |
|
1999 |
264 |
1-2 |
p. 74-80 7 p. |
artikel |
22 |
Low temperature pressureless sintering of sol-gel derived mullite
|
Amutharani, D |
|
1999 |
264 |
1-2 |
p. 254-261 8 p. |
artikel |
23 |
Mechanical stability and electrical conductivity of Cu–Ag filamentary microcomposites
|
Hong, Sun Ig |
|
1999 |
264 |
1-2 |
p. 151-158 8 p. |
artikel |
24 |
Microstructural evolution in the phase mixtures of Ti(C,N)–Mo at 1600°C
|
Qian, Ma |
|
1999 |
264 |
1-2 |
p. 39-46 8 p. |
artikel |
25 |
Numerical simulation of tensile tests of prestrained sheets
|
Menezes, L.F |
|
1999 |
264 |
1-2 |
p. 130-138 9 p. |
artikel |
26 |
Phase transformations and strengthening during ageing of CuNi10Al3 alloy
|
Sierpiński, Zdzisław |
|
1999 |
264 |
1-2 |
p. 279-285 7 p. |
artikel |
27 |
Plastic deformation of nanocrystalline Cu and Cu–0.2 wt.% B
|
Suryanarayanan Iyer, R |
|
1999 |
264 |
1-2 |
p. 210-214 5 p. |
artikel |
28 |
The development of Fe–Zn intermetallic compounds in solid Fe/Zn and Fe/Zn–Al diffusion couples during short-term annealing at 400°C
|
Syahbuddin, |
|
1999 |
264 |
1-2 |
p. 201-209 9 p. |
artikel |
29 |
The effect of compressive deformation of austenite on the Widmanstätten ferrite transformation in Fe–Mn–Si–C steel
|
Larn, R.H |
|
1999 |
264 |
1-2 |
p. 139-150 12 p. |
artikel |
30 |
The incorporation of ceramic particles in molten aluminium and the relationship to contact angle data
|
Kennedy, A.R |
|
1999 |
264 |
1-2 |
p. 122-129 8 p. |
artikel |
31 |
Thermal residual stresses in NiAl–AlN–Al2O3 composites measured by neutron diffraction
|
Choo, Hahn |
|
1999 |
264 |
1-2 |
p. 108-121 14 p. |
artikel |
32 |
Transformation conditions in an Fe-based shape memory alloy under tensile–torsional loads: martensite start surface and austenite start/finish planes
|
Nishimura, Fumihito |
|
1999 |
264 |
1-2 |
p. 232-244 13 p. |
artikel |