nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Aging behaviour of Ti15Mo5Zr and Ti15Mo5Zr3Al alloy up to 573 K
|
Komatsu, Shin-ya |
|
1996 |
213 |
1-2 |
p. 61-65 5 p. |
artikel |
2 |
Analysis of microfracture mechanism of titanium alloy by acoustic emission technique
|
Mashino, S. |
|
1996 |
213 |
1-2 |
p. 66-70 5 p. |
artikel |
3 |
An overview on the development of titanium alloys for non-aerospace application in Japan
|
Yamada, Makoto |
|
1996 |
213 |
1-2 |
p. 8-15 8 p. |
artikel |
4 |
An overview on the use of titanium in the aerospace industry
|
Boyer, R.R. |
|
1996 |
213 |
1-2 |
p. 103-114 12 p. |
artikel |
5 |
Application of heat-resistant titanium-based compressor disk with dual structure
|
Nishikiori, S. |
|
1996 |
213 |
1-2 |
p. 124-127 4 p. |
artikel |
6 |
Corrosion resistance and corrosion fatigue strength of new titanium alloys for medical implants without V and Al
|
Okazaki, Yoshimitsu |
|
1996 |
213 |
1-2 |
p. 138-147 10 p. |
artikel |
7 |
Development of near-β high strength Ti alloy Ti-5Al-2Sn-4Zr-3Cr-3Mo with superior fatigue crack growth properties
|
Matsumoto, Toshio |
|
1996 |
213 |
1-2 |
p. 154-156 3 p. |
artikel |
8 |
Fracture characteristics analysis related to the microstructures in titanium alloys
|
Niinomi, M. |
|
1996 |
213 |
1-2 |
p. 16-24 9 p. |
artikel |
9 |
General creep characteristics of α 2 single-phase polycrystalline intermetallics
|
Nagae, Yuji |
|
1996 |
213 |
1-2 |
p. 32-36 5 p. |
artikel |
10 |
Hard surfacing of TiAl intermetallic compound by plasma carburization
|
Noda, T. |
|
1996 |
213 |
1-2 |
p. 157-161 5 p. |
artikel |
11 |
High temperature strength of α TiAl alloys with a locally ordered structure
|
Koike, J. |
|
1996 |
213 |
1-2 |
p. 98-102 5 p. |
artikel |
12 |
Issues and breakthrough in the manufacture of turboengine titanium parts
|
Honnorat, Yves |
|
1996 |
213 |
1-2 |
p. 115-123 9 p. |
artikel |
13 |
Low-cycle fatigue behavior of commercially pure titanium
|
Takao, Kenichi |
|
1996 |
213 |
1-2 |
p. 81-85 5 p. |
artikel |
14 |
Mechanical properties of a Ti15V3Cr3Sn3Al alloy affected by the impurity hydrogen
|
Itoh, Goroh |
|
1996 |
213 |
1-2 |
p. 93-97 5 p. |
artikel |
15 |
Microstructure and properties of titanium alloy produced in the newly developed blended elemental powder metallurgy process
|
Fujita, Takahiro |
|
1996 |
213 |
1-2 |
p. 148-153 6 p. |
artikel |
16 |
Microstructure development in a thermomechanically processed Ti15V3Cr3Sn3Al alloy
|
Makino, T. |
|
1996 |
213 |
1-2 |
p. 51-60 10 p. |
artikel |
17 |
New high strength titanium alloy Ti10%Zr for spectacle frames
|
Nakasuji, Kazuyuki |
|
1996 |
213 |
1-2 |
p. 162-165 4 p. |
artikel |
18 |
Preface
|
|
|
1996 |
213 |
1-2 |
p. ix- 1 p. |
artikel |
19 |
Processing, microstructure, and properties of β-CEZ
|
Peters, J.O. |
|
1996 |
213 |
1-2 |
p. 71-80 10 p. |
artikel |
20 |
Recent progress in our understanding of deformation and fracture of two-phase and single-phase TiAl alloys
|
Yamaguchi, M. |
|
1996 |
213 |
1-2 |
p. 25-31 7 p. |
artikel |
21 |
Single-phase interdiffusion in TiAl and Ti3Al intermetallic compounds
|
Sprengel, W. |
|
1996 |
213 |
1-2 |
p. 45-50 6 p. |
artikel |
22 |
Status of investment cast gamma titanium aluminides in the USA
|
Larsen Jr., Donald E. |
|
1996 |
213 |
1-2 |
p. 128-133 6 p. |
artikel |
23 |
The microstructure dependence of fatigue behaviour in Ti15Mo5Zr3Al alloy
|
Tokaji, Keiro |
|
1996 |
213 |
1-2 |
p. 86-92 7 p. |
artikel |
24 |
The role of intermetallic precipitates in Ti-62222S
|
Evans, Daniel J. |
|
1996 |
213 |
1-2 |
p. 37-44 8 p. |
artikel |
25 |
The state of the USA titanium industry in 1995
|
Seagle, Stan R. |
|
1996 |
213 |
1-2 |
p. 1-7 7 p. |
artikel |
26 |
The use of titanium for medical applications in the USA
|
Wang, Kathy |
|
1996 |
213 |
1-2 |
p. 134-137 4 p. |
artikel |