nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Effect of the electrical discharge machining on strength and reliability of TiN/Si3N4 composites
|
Liu, Chien-Cheng |
|
2003 |
29 |
6 |
p. 679-687 9 p. |
artikel |
2 |
Effect of the microstructure on the mechanical properties of CaO–P2O5–SiO2–MgO–F− glass ceramics
|
Yu, Bing |
|
2003 |
29 |
6 |
p. 695-698 4 p. |
artikel |
3 |
Effect of Y2O3 addition on ammono sol–gel synthesis and sintering of Si3N4–SiC nanocomposite powder
|
Gao, Jiming |
|
2003 |
29 |
6 |
p. 655-661 7 p. |
artikel |
4 |
Erosion characteristics of silicon nitride ceramics
|
Choi, Hyeon-Ju |
|
2003 |
29 |
6 |
p. 713-719 7 p. |
artikel |
5 |
Growth and characterization of dumbbell-shaped MgO nanowhiskers
|
Chen, Yongjun |
|
2003 |
29 |
6 |
p. 663-666 4 p. |
artikel |
6 |
Heat and mass transfer models in convection drying of clay slabs
|
Sander, Aleksandra |
|
2003 |
29 |
6 |
p. 641-653 13 p. |
artikel |
7 |
Joining of sapphire and hot pressed Al2O3 using Ag70.5Cu27.5Ti2 brazing filler metal
|
Ning, Honglong |
|
2003 |
29 |
6 |
p. 689-694 6 p. |
artikel |
8 |
Low-temperature fabrication of anorthite ceramics from kaolinite and calcium carbonate with boron oxide addition
|
Mergen, Ayhan |
|
2003 |
29 |
6 |
p. 667-670 4 p. |
artikel |
9 |
Materials synthesis and characterization of 8YSZ nanomaterials for the fabrication of electrolyte membranes in solid oxide fuel cells
|
Menzler, Norbert H. |
|
2003 |
29 |
6 |
p. 619-628 10 p. |
artikel |
10 |
Microstructures and mechanical properties of Sr2Nb2O7-toughened 3Y-TZP ceramics
|
Liu, X.Q. |
|
2003 |
29 |
6 |
p. 635-640 6 p. |
artikel |
11 |
Microstructures of refractory castables prepared with sol–gel additives
|
Ghosh, S. |
|
2003 |
29 |
6 |
p. 671-677 7 p. |
artikel |
12 |
Preparation and characterizations of Zn2SiO4:Mn green phosphors
|
Cho, Tae Hwan |
|
2003 |
29 |
6 |
p. 611-618 8 p. |
artikel |
13 |
Processing and characterization of bioglass reinforced hydroxyapatite composites
|
Goller, Gultekin |
|
2003 |
29 |
6 |
p. 721-724 4 p. |
artikel |
14 |
The effect of starting powder on the microstructure development of alumina–aluminum titanate composites
|
Park, Sang-Yeup |
|
2003 |
29 |
6 |
p. 707-712 6 p. |
artikel |
15 |
The influence of pH and temperature on the morphology of hydroxyapatite synthesized by hydrothermal method
|
Liu, Jingbing |
|
2003 |
29 |
6 |
p. 629-633 5 p. |
artikel |
16 |
The influence of the microstructure on the hardness of sintered hydroxyapatite
|
Hoepfner, Timothy P |
|
2003 |
29 |
6 |
p. 699-706 8 p. |
artikel |
17 |
Thermal shock behaviour of mullite ceramic
|
Hamidouche, M |
|
2003 |
29 |
6 |
p. 599-609 11 p. |
artikel |