nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A detailed study of thermal degradation of poly(2-hydroxyethyl methacrylate)
|
Demirelli, Kadir |
|
2001 |
72 |
1 |
p. 75-80 6 p. |
artikel |
2 |
An investigation of the potential for chemical modification and subsequent polymeric grafting as a means of protecting wood against photodegradation
|
Hill, Callum A.S |
|
2001 |
72 |
1 |
p. 133-139 7 p. |
artikel |
3 |
Characterization and reprocessing of greenhouse films
|
Tzankova Dintcheva, N. |
|
2001 |
72 |
1 |
p. 141-146 6 p. |
artikel |
4 |
Chemical and morphologial modifications of irradiated linear low density polyethylene (LLDPE)
|
Guadagno, Liberata |
|
2001 |
72 |
1 |
p. 175-186 12 p. |
artikel |
5 |
Corrigendum to “A representation of the autoacceleration stage of polypropylene thermooxidation in reduced coordinates” [Polym Degrad Stab 2000;67(1):49–56]
|
Tiemblo, Pilar |
|
2001 |
72 |
1 |
p. 187- 1 p. |
artikel |
6 |
Degradable polyurethanes containing poly(butylene succinate) and poly(ethylene glycol)
|
Lee, Sung-Il |
|
2001 |
72 |
1 |
p. 81-87 7 p. |
artikel |
7 |
Determination of ultraviolet light absorber longevity and distribution in automotive paint systems using ultraviolet micro-spectroscopy
|
Smith, C.A. |
|
2001 |
72 |
1 |
p. 89-97 9 p. |
artikel |
8 |
Dynamic mechanical analysis and Vickers micro hardness correlation for polymer coating UV ageing characterisation
|
Bartolomeo, P. |
|
2001 |
72 |
1 |
p. 63-68 6 p. |
artikel |
9 |
Electron-beam irradiation of poly(vinyl chloride)/epoxidized natural rubber blend in the presence of Irganox 1010
|
Ratnam, Chantara Thevy |
|
2001 |
72 |
1 |
p. 147-155 9 p. |
artikel |
10 |
Evaluation of accelerated weathering tests for three paint systems: a comparative study of their aging behaviour
|
Perrin, F.X |
|
2001 |
72 |
1 |
p. 115-124 10 p. |
artikel |
11 |
Factors affecting the adsorption of stabilisers on to carbon black (flow micro-calorimetry studies) 4. Secondary antioxidants
|
Peña, J.M |
|
2001 |
72 |
1 |
p. 31-45 15 p. |
artikel |
12 |
Heterogeneous features of autooxidation of hydrocarbon polymers
|
Mikheev, Yu.A. |
|
2001 |
72 |
1 |
p. 1-21 21 p. |
artikel |
13 |
2-Hydroxybenzophenone UV-absorber containing 4,4,5,5-tetramethylimidazolidine fragment
|
Zakrzewski, Jerzy |
|
2001 |
72 |
1 |
p. 109-113 5 p. |
artikel |
14 |
Initial degradation processes of cellulose at elevated temperatures revisited — chemiluminescence evidence
|
Strlic̆, Matija |
|
2001 |
72 |
1 |
p. 157-162 6 p. |
artikel |
15 |
Interactions between carbon black and stabilisers in LDPE thermal oxidation
|
Peña, J.M. |
|
2001 |
72 |
1 |
p. 163-174 12 p. |
artikel |
16 |
New stabilisers for polymers on the basis of IPDI protected 2,2-thiobis(4-methyl-6-tert-butylphenol) and hindered amines
|
Ahmad, S |
|
2001 |
72 |
1 |
p. 47-51 5 p. |
artikel |
17 |
On the compatibility of polysaccharide/maleic copolymer blends I. Thermal behaviour of dextran containing blends
|
Bumbu, Gina-Gabriela |
|
2001 |
72 |
1 |
p. 99-108 10 p. |
artikel |
18 |
Organic thermal stabilizers for rigid poly(vinyl chloride) III. Crotonal and cinnamal thiobarbituric acids
|
Mohamed, N.A. |
|
2001 |
72 |
1 |
p. 53-61 9 p. |
artikel |
19 |
Preparation and thermal degradation of poly(p-substituted phenacyl methacrylates)
|
Coşkun, Mehmet |
|
2001 |
72 |
1 |
p. 69-74 6 p. |
artikel |
20 |
The autoacceleration of polypropylene thermo-oxidation in reduced coordinates: effect of the oxidation temperature and of polyolefin structure
|
Tiemblo, P |
|
2001 |
72 |
1 |
p. 23-30 8 p. |
artikel |
21 |
Thermal degradation of thermoplastic and thermosetting polymers induced by laser radiation and its study by FTIR spectroscopy
|
Bormashenko, Edward |
|
2001 |
72 |
1 |
p. 125-131 7 p. |
artikel |