1 |
A kinetic model of polymer degradation during extrusion
|
El'darov, E.G. |
|
1996 |
51 |
3 |
p. 271-279 9 p. |
artikel |
2 |
Calendar of events
|
|
|
1996 |
51 |
3 |
p. 367-368 2 p. |
artikel |
3 |
Contents of volume 51
|
|
|
1996 |
51 |
3 |
p. 369-371 3 p. |
artikel |
4 |
Degradation of polyacrylamide in dilute solution
|
Rho, Taeho |
|
1996 |
51 |
3 |
p. 287-293 7 p. |
artikel |
5 |
Degradation of PVC: Effect of zinc chloride on the concentration of polyenes
|
Manzoor, W. |
|
1996 |
51 |
3 |
p. 295-299 5 p. |
artikel |
6 |
Effect of bis(dithiocarbamato)copper(II) complexes on the photo-degradation of poly(vinyl chloride)
|
Jeliazkowa, Bojana |
|
1996 |
51 |
3 |
p. 301-305 5 p. |
artikel |
7 |
Effects of gamma-irradiation on copolymers of phenyl methacrylate and methyl methacrylate
|
Zulfiqar, Mohammad |
|
1996 |
51 |
3 |
p. 327-333 7 p. |
artikel |
8 |
Evaluation of biodegradabilities of biosynthetic and chemosynthetic polyesters in river water
|
Doi, Yoshiharu |
|
1996 |
51 |
3 |
p. 281-286 6 p. |
artikel |
9 |
Hydrolytic degradation of peroxide modified poly(L-lactide)
|
Södergård, Anders |
|
1996 |
51 |
3 |
p. 351-359 9 p. |
artikel |
10 |
New type of ecologically safe flame retardant based on polymer char former
|
Lomakin, S.M. |
|
1996 |
51 |
3 |
p. 343-350 8 p. |
artikel |
11 |
Polymer-analogous conversions of olefin and diene oligomers as an advanced way of synthesizing stabilizers for halogen-containing polymers
|
Biglova, R.Z. |
|
1996 |
51 |
3 |
p. 251-264 14 p. |
artikel |
12 |
The influence of stability of raw materials used in sizings for E and AR fiberglass manufacture
|
Ramos, Guadalupe |
|
1996 |
51 |
3 |
p. 361-365 5 p. |
artikel |
13 |
The mathematical modeling of the inhibition mechanisms of sterically-hindered phenols in oxidizing low-density polyethylene melt
|
Kharitonov, V.V. |
|
1996 |
51 |
3 |
p. 335-341 7 p. |
artikel |
14 |
Thermal decomposition behaviour of polyamide fire-retardant compositions containing magnesium hydroxide filler
|
Hornsby, P.R. |
|
1996 |
51 |
3 |
p. 235-249 15 p. |
artikel |
15 |
Thermal degradation of bismaleimide and bisnadimide networks—products of thermal degradation and type of crosslinking points
|
Torrecillas, R. |
|
1996 |
51 |
3 |
p. 307-318 12 p. |
artikel |
16 |
Thermal degradation studies of poly(ethylene glycol allenyl-methyl ether)s and their copolymers with styrene
|
Aggour, Y.A. |
|
1996 |
51 |
3 |
p. 265-269 5 p. |
artikel |
17 |
The thermal degradation of copolymers of glycidyl methacrylate and vinylacetate
|
Piracha, Asifa |
|
1996 |
51 |
3 |
p. 319-326 8 p. |
artikel |