nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Acoustic emission characterization of the fracture mechanism of a high compliant, glass-matrix composite
|
Takeda, N. |
|
1991 |
40 |
4-5 |
p. 791-799 9 p. |
artikel |
2 |
Alumina coating of austenitic stainless steel by sol-gel process
|
Miyazawa, Kun'ichi |
|
1991 |
40 |
4-5 |
p. 967-973 7 p. |
artikel |
3 |
Application of ultrasound on joining of ceramics to metals
|
Naka, M. |
|
1991 |
40 |
4-5 |
p. 951-956 6 p. |
artikel |
4 |
Assuring reliability of advanced materials in severe applications
|
Prager, Martin |
|
1991 |
40 |
4-5 |
p. 921-926 6 p. |
artikel |
5 |
Characterization of high temperature creep crack growth and creep life from high temperature ductile through to high temperature brittle materials
|
Yokobori Jr., A.Toshimitsu |
|
1991 |
40 |
4-5 |
p. 737-748 12 p. |
artikel |
6 |
Crack propagation behavior of sintered silicon nitride under cyclic loads of high stress ratio and high frequency
|
Ueno, A. |
|
1991 |
40 |
4-5 |
p. 913-920 8 p. |
artikel |
7 |
Creep crack growth in high temperature ductile materials
|
Saxena, Ashok |
|
1991 |
40 |
4-5 |
p. 721-736 16 p. |
artikel |
8 |
Damage induced in sic by a particle impact
|
Maekawa, Ichiro |
|
1991 |
40 |
4-5 |
p. 879-886 8 p. |
artikel |
9 |
Dynamic fracture toughness in ceramics and ceramics matrix composites
|
Kishi, T. |
|
1991 |
40 |
4-5 |
p. 785-790 6 p. |
artikel |
10 |
Editorial: Software survey section
|
|
|
1991 |
40 |
4-5 |
p. I-III nvt p. |
artikel |
11 |
Effect of cooling configuration on thermal shock fracture toughness of SiC
|
Kanto, Y. |
|
1991 |
40 |
4-5 |
p. 893-901 9 p. |
artikel |
12 |
Fatigue crack propagation of Sic whisker reinforced 6061 aluminum alloy composite
|
Ishii, Hitoshi |
|
1991 |
40 |
4-5 |
p. 821-827 7 p. |
artikel |
13 |
Fracture and fatigue of high performance composite materials: mechanisms and prediction
|
Bathias, Claude |
|
1991 |
40 |
4-5 |
p. 757-783 27 p. |
artikel |
14 |
Fracture toughness and acoustic emission behavior of dental composite resins
|
Kim, Kyo-Han |
|
1991 |
40 |
4-5 |
p. 811-819 9 p. |
artikel |
15 |
High-temperature deformation and grain growth in fine-grained zirconia
|
Yoshizawa, Yu-Ichi |
|
1991 |
40 |
4-5 |
p. 847-854 8 p. |
artikel |
16 |
Inelastic deformation of bioactive glass-ceramics
|
Hirao, Kazuyuki |
|
1991 |
40 |
4-5 |
p. 837-842 6 p. |
artikel |
17 |
Interface microstructure and strength of SiC/SiC joint brazed with CuTi alloys
|
Nishino, Toshitsugu |
|
1991 |
40 |
4-5 |
p. 829-836 8 p. |
artikel |
18 |
Interfacial phenomena in joining of ceramics by active metal brazing alloy
|
Chung, Y.S. |
|
1991 |
40 |
4-5 |
p. 941-949 9 p. |
artikel |
19 |
Internal crack initiation in high cycle fatigue at cryogenic temperatures
|
Nagai, K. |
|
1991 |
40 |
4-5 |
p. 957-965 9 p. |
artikel |
20 |
Joining of zirconia to metals using Zr-Cu alloy
|
Iwamoto, Nobuya |
|
1991 |
40 |
4-5 |
p. 931-940 10 p. |
artikel |
21 |
Localized viscoplasticity in structural ceramics: Modelling and influence on mechanical properties
|
Boussuge, Michel |
|
1991 |
40 |
4-5 |
p. 855-861 7 p. |
artikel |
22 |
Microstructure dependence of mechanical and dielectric strengths—i. porosity
|
Kishimoto, Akira |
|
1991 |
40 |
4-5 |
p. 927-930 4 p. |
artikel |
23 |
New computing systems and their impact on structural and fracture mechanics calculations
|
Liebowitz, Harold |
|
1991 |
40 |
4-5 |
p. 687-704 18 p. |
artikel |
24 |
Oblique impact damage by spherical particles onto Si3N4
|
Akimune, Yoshio |
|
1991 |
40 |
4-5 |
p. 887-892 6 p. |
artikel |
25 |
Phenomenon of intergranular cavitation and failure in superplasticity
|
Lee, Ho-Sung |
|
1991 |
40 |
4-5 |
p. 843-846 4 p. |
artikel |
26 |
Preface
|
|
|
1991 |
40 |
4-5 |
p. vii- 1 p. |
artikel |
27 |
Quasi-brittle behaviour of ceramics and its relevance for thermal shock
|
Swain, Michael V. |
|
1991 |
40 |
4-5 |
p. 871-877 7 p. |
artikel |
28 |
Relaxation behaviour of Hastelloy XR in LCF tests
|
Kikuchi, K. |
|
1991 |
40 |
4-5 |
p. 749-755 7 p. |
artikel |
29 |
Some critical questions and future directions for fracture research
|
Yokobori, Takeo |
|
1991 |
40 |
4-5 |
p. 705-720 16 p. |
artikel |
30 |
Static and cyclic fatigue of glass and silicon nitride under tensile and tension-compression fatigue tests
|
Otsuka, Akio |
|
1991 |
40 |
4-5 |
p. 903-911 9 p. |
artikel |
31 |
Time-dependent mechanical behaviour of alumina ceramics
|
Yokobori Jr., A.T. |
|
1991 |
40 |
4-5 |
p. 863-870 8 p. |
artikel |
32 |
Transformed Zro2 volume fraction in Al2o3 matrix multi-toughening composites
|
Ikeda, Koji |
|
1991 |
40 |
4-5 |
p. 801-809 9 p. |
artikel |