Effect of Cobalt Content on the Oxidation and Corrosion Behavior of Ni–Fe-Based Superalloy for Ultra-Supercritical Boiler Applications
|
Lu, Jintao |
|
2017 |
89 |
1-2 |
p. 197-209 |
artikel |
2 |
Effect of Dilute Tellurium and Selenium Additions on the High-Temperature Oxidation Resistance of Copper Alloys
|
Huang, Ruijie |
|
2017 |
89 |
1-2 |
p. 141-149 |
artikel |
3 |
Effect of Water Density/Pressure on the Corrosion Behavior of 304 and 310 Stainless Steels
|
Sanchez, Rainier Garcia |
|
2017 |
89 |
1-2 |
p. 165-182 |
artikel |
4 |
Fume Formation from Oxidation of Liquid SiMn Alloy
|
Ma, Yan |
|
2017 |
89 |
1-2 |
p. 211-231 |
artikel |
5 |
High-Temperature Oxidation and Pickling Behaviour of HSLA Steels
|
Gutierrez-Platas, J. L. |
|
2018 |
89 |
1-2 |
p. 33-48 |
artikel |
6 |
High-Temperature Oxidation Behavior of SIMP Steel at 800 °C
|
Shi, Quanqiang |
|
2017 |
89 |
1-2 |
p. 49-60 |
artikel |
7 |
Influence of Alloying Elements on the Behavior of Different Ferritic Steels as Candidate Materials for SOFC Interconnect
|
Garcia-Fresnillo, L. |
|
2017 |
89 |
1-2 |
p. 61-80 |
artikel |
8 |
Influence of Preoxidation on High-Temperature Corrosion of a FeCrAl Alloy Under Conditions Relevant to Biomass Firing
|
Okoro, Sunday Chukwudi |
|
2017 |
89 |
1-2 |
p. 99-122 |
artikel |
9 |
Microstructure, Chemical- and Phase Composition of Sanicro 25 Austenitic Steel After Oxidation in Steam at 700 °C
|
Rutkowski, B. |
|
2017 |
89 |
1-2 |
p. 183-195 |
artikel |
10 |
Oxidation Behaviour of Alloys 800H, 3033 and 304 in High-Temperature Supercritical Water
|
Bsat, Suzan |
|
2017 |
89 |
1-2 |
p. 151-163 |
artikel |
11 |
Reduction of Wustite Scale by Dissolved Carbon in Steel at 650–900 °C
|
Chen, R. Y. |
|
2017 |
89 |
1-2 |
p. 1-31 |
artikel |
12 |
The Effect of Metallic Co-Coating Thickness on Ferritic Stainless Steels Intended for Use as Interconnect Material in Intermediate Temperature Solid Oxide Fuel Cells
|
Falk-Windisch, Hannes |
|
2017 |
89 |
1-2 |
p. 233-250 |
artikel |
13 |
The Effect of Sulfur on the Carburization of Three Fe–19Ni–21Cr–xAl (x = 0, 2, 6 at.%) Alloys at 900 °C in Oxygen-Contaminated CH4–H2–H2S Atmospheres
|
Liu, S. |
|
2017 |
89 |
1-2 |
p. 279-301 |
artikel |
14 |
The Effect of Temperature on the Formation of Oxide Scales Regarding Commercial Superheater Steels
|
Lehmusto, J. |
|
2017 |
89 |
1-2 |
p. 251-278 |
artikel |
15 |
The Transition from Transient Oxide to Protective Al2O3 Scale on Fe–Cr–Al Alloys During Heating to 1000 °C
|
Yoneda, Suzue |
|
2017 |
89 |
1-2 |
p. 81-97 |
artikel |
16 |
ToF-SIMS Study on the Initial Stages of the Halogen Effect in the Oxidation of TiAl Alloys
|
Friedle, S. |
|
2017 |
89 |
1-2 |
p. 123-139 |
artikel |