nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A cellular automaton model for predicting intergranular corrosion
|
Lishchuk, S.V. |
|
2011 |
53 |
8 |
p. 2518-2526 9 p. |
artikel |
2 |
A generic statistical methodology to predict the maximum pit depth of a localized corrosion process
|
Jarrah, A. |
|
2011 |
53 |
8 |
p. 2453-2467 15 p. |
artikel |
3 |
An investigation on the role of texture and surface morphology in the corrosion resistance of zinc electrodeposits
|
Khorsand, S. |
|
2011 |
53 |
8 |
p. 2676-2678 3 p. |
artikel |
4 |
Chlorhexidine digluconate as corrosion inhibitor for carbon steel dissolution in emulsified diesel fuel
|
Deyab, M.A. |
|
2011 |
53 |
8 |
p. 2592-2597 6 p. |
artikel |
5 |
Combined effect of resistance spot welding and post-welding sensitization on the degree of sensitization of AISI 304 stainless steel
|
De Tiedra, Pilar |
|
2011 |
53 |
8 |
p. 2670-2675 6 p. |
artikel |
6 |
Corrosion behavior of a cerium-based conversion coating on alumina borate whisker-reinforced AA6061 composite pre-treated by hydrogen fluoride
|
Tang, S.W. |
|
2011 |
53 |
8 |
p. 2636-2644 9 p. |
artikel |
7 |
Corrosion mechanism of Mo/Nd16Fe71B13/Mo film in a simulated marine atmosphere
|
Li, Chunling |
|
2011 |
53 |
8 |
p. 2549-2557 9 p. |
artikel |
8 |
Corrosion of Ti3AlC2 at 800–1100°C in Ar–0.2% SO2 gas atmosphere
|
Lee, Dong Bok |
|
2011 |
53 |
8 |
p. 2645-2650 6 p. |
artikel |
9 |
Effect of alternately changing the dissolved Ni ion concentration on the oxidation of 304 stainless steel in oxygenated high temperature water
|
Kuang, Wenjun |
|
2011 |
53 |
8 |
p. 2582-2591 10 p. |
artikel |
10 |
Effect of hydrogen on the properties and fracture characteristics of TRIP 800 steels
|
Sojka, J. |
|
2011 |
53 |
8 |
p. 2575-2581 7 p. |
artikel |
11 |
Effect of the micro-plasma arc welding technique on the microstructure and pitting corrosion of AISI 316L stainless steels in heavy LiBr brines
|
Sánchez-Tovar, R. |
|
2011 |
53 |
8 |
p. 2598-2610 13 p. |
artikel |
12 |
Effects of shielding gases on the microstructure and localized corrosion of tube-to-tube sheet welds of super austenitic stainless steel for seawater cooled condenser
|
Kim, Soon-Tae |
|
2011 |
53 |
8 |
p. 2611-2618 8 p. |
artikel |
13 |
Exfoliation corrosion of extruded 2024-T4 in the coastal environments in China
|
Sun, Shuangqing |
|
2011 |
53 |
8 |
p. 2527-2538 12 p. |
artikel |
14 |
Hydrogen uptake in austenitic stainless steels by exposure to gaseous hydrogen and its effect on tensile deformation
|
Mine, Yoji |
|
2011 |
53 |
8 |
p. 2619-2629 11 p. |
artikel |
15 |
Influence of anions on the formation and structure of artificial zinc rusts
|
Tanaka, Hidekazu |
|
2011 |
53 |
8 |
p. 2502-2507 6 p. |
artikel |
16 |
Influence of phosphate species on green rust I transformation and local structure and morphology of γ-FeOOH
|
Sahoo, Gadadhar |
|
2011 |
53 |
8 |
p. 2446-2452 7 p. |
artikel |
17 |
Inhibition of the corrosion of steel in hydrochloric acid solution by some organic molecules containing the methylthiophenyl moiety
|
Nataraja, S.E. |
|
2011 |
53 |
8 |
p. 2651-2659 9 p. |
artikel |
18 |
Localisation of oxygen reduction sites in the case of iron long term atmospheric corrosion
|
Monnier, Judith |
|
2011 |
53 |
8 |
p. 2468-2473 6 p. |
artikel |
19 |
Mechanisms of the dechlorination of iron archaeological artefacts extracted from seawater
|
Kergourlay, F. |
|
2011 |
53 |
8 |
p. 2474-2483 10 p. |
artikel |
20 |
Microstructure of oxides in thermal barrier coatings grown under dry/humid atmosphere
|
Zhou, Zhaohui |
|
2011 |
53 |
8 |
p. 2630-2635 6 p. |
artikel |
21 |
Molten salt synthesis of perovskite conversion coatings: A novel approach for corrosion protection of stainless steels in molten carbonate fuel cells
|
Frangini, S. |
|
2011 |
53 |
8 |
p. 2539-2548 10 p. |
artikel |
22 |
Numerical simulation of the effect of grain size on corrosion processes: Surface roughness oscillation and cluster detachment
|
Taleb, A. |
|
2011 |
53 |
8 |
p. 2508-2513 6 p. |
artikel |
23 |
Oxidation kinetics of polyacrylonitrile-based carbon fibers in air and the effect on their tensile properties
|
Tong, Yuanjian |
|
2011 |
53 |
8 |
p. 2484-2488 5 p. |
artikel |
24 |
Pitting corrosion of intermetallic compound Ni3(Si,Ti) in sodium chloride solutions
|
Wagle, Sanat |
|
2011 |
53 |
8 |
p. 2514-2517 4 p. |
artikel |
25 |
Role of Bayer solution concentration and temperature in stress corrosion cracking susceptibility of steel
|
Pal, Sarvesh |
|
2011 |
53 |
8 |
p. 2660-2669 10 p. |
artikel |
26 |
Sharpening behaviour of W-wire electrodes in 10–25wt.% NaOH solutions
|
Huang, Ching An |
|
2011 |
53 |
8 |
p. 2566-2574 9 p. |
artikel |
27 |
Stress corrosion cracking of uni-directionally cold worked 316NG stainless steel in simulated PWR primary water with various dissolved hydrogen concentrations
|
Meng, Fanjiang |
|
2011 |
53 |
8 |
p. 2558-2565 8 p. |
artikel |
28 |
The effect of two oleo-gum resin exudate from Ferula assa-foetida and Dorema ammoniacum on mild steel corrosion in acidic media
|
Behpour, M. |
|
2011 |
53 |
8 |
p. 2489-2501 13 p. |
artikel |
29 |
Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn–Al–Mg coatings on steel
|
Volovitch, P. |
|
2011 |
53 |
8 |
p. 2437-2445 9 p. |
artikel |