nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
A fundamental study of Fe–Cr binary alloy–oxide film interfaces at 288°C by computational chemistry calculations
|
Das, Nishith Kumar |
|
2010 |
52 |
7 |
p. 2349-2352 4 p. |
artikel |
2 |
Artificial neural networks for pitting potential prediction of resistance spot welding joints of AISI 304 austenitic stainless steel
|
Martín, Óscar |
|
2010 |
52 |
7 |
p. 2397-2402 6 p. |
artikel |
3 |
Corrosion behaviour of stainless steels in aqueous solutions of methanesulfonic acid
|
Finšgar, Matjaž |
|
2010 |
52 |
7 |
p. 2430-2438 9 p. |
artikel |
4 |
Corrosion behaviour of vacuum induction-melted Ni-based alloy in sulphuric acid
|
Chang, J.H. |
|
2010 |
52 |
7 |
p. 2323-2330 8 p. |
artikel |
5 |
Corrosion behaviour of Y2O3–ZrO2 coatings on IN713LC in a LiCl–Li2O molten salt
|
Cho, Soo-Haeng |
|
2010 |
52 |
7 |
p. 2353-2364 12 p. |
artikel |
6 |
Corrosion diary
|
|
|
2010 |
52 |
7 |
p. I- 1 p. |
artikel |
7 |
Corrosion inhibition of carbon steel in hydrochloric acid solution by fruit peel aqueous extracts
|
da Rocha, Janaina Cardozo |
|
2010 |
52 |
7 |
p. 2341-2348 8 p. |
artikel |
8 |
Corrosion resistance of welds in type 304L stainless steel made with a nickel–copper–ruthenium welding consumable
|
Liang, D. |
|
2010 |
52 |
7 |
p. 2439-2451 13 p. |
artikel |
9 |
Degradation of the corrosion resistance of anodic oxide films through immersion in the anodising electrolyte
|
García-Rubio, M. |
|
2010 |
52 |
7 |
p. 2219-2227 9 p. |
artikel |
10 |
Detection of breakaway oxidation with Acoustic Emission during titanium oxide scale growth
|
Tran, Minh-Thi |
|
2010 |
52 |
7 |
p. 2365-2371 7 p. |
artikel |
11 |
Effect of Ca2+and Mg2+ on corrosion and scaling of galvanized steel pipe in simulated geothermal water
|
Wu, Kun-hu |
|
2010 |
52 |
7 |
p. 2244-2249 6 p. |
artikel |
12 |
Electrochemical corrosion behaviour of Bi–11Ag alloy for electronic packaging applications
|
Song, Jenn-Ming |
|
2010 |
52 |
7 |
p. 2519-2524 6 p. |
artikel |
13 |
Electrochemical polarization behavior of X70 steel in thin carbonate/bicarbonate solution layers trapped under a disbonded coating and its implication on pipeline SCC
|
Fu, A.Q. |
|
2010 |
52 |
7 |
p. 2511-2518 8 p. |
artikel |
14 |
Empirical model for dissolved oxygen depletion during corrosion of drinking water copper pipes
|
Vargas, Ignacio T. |
|
2010 |
52 |
7 |
p. 2250-2257 8 p. |
artikel |
15 |
Growth characteristics and corrosion resistance of micro-arc oxidation coating on pure magnesium for biomedical applications
|
Zhao, Lichen |
|
2010 |
52 |
7 |
p. 2228-2234 7 p. |
artikel |
16 |
High temperature corrosion behaviour of a gradient NiCoCrAlYSi coating II: Oxidation and hot corrosion
|
Jiang, S.M. |
|
2010 |
52 |
7 |
p. 2316-2322 7 p. |
artikel |
17 |
H2S and O2 influence on the corrosion of carbon steel immersed in a solution containing 3M diethanolamine
|
Garcia-Arriaga, V. |
|
2010 |
52 |
7 |
p. 2268-2279 12 p. |
artikel |
18 |
Influence of second phases on the electrochemical behavior of hot dipped Al–Mg–Si coated steel
|
Kruehong, Chaiyaput |
|
2010 |
52 |
7 |
p. 2379-2386 8 p. |
artikel |
19 |
Investigations of corrosion films formed on API-X52 pipeline steel in acid sour media
|
Hernández-Espejel, A. |
|
2010 |
52 |
7 |
p. 2258-2267 10 p. |
artikel |
20 |
Magnesium secondary alloys: Alloy design for magnesium alloys with improved tolerance limits against impurities
|
Blawert, C. |
|
2010 |
52 |
7 |
p. 2452-2468 17 p. |
artikel |
21 |
Microstructural analysis and corrosion behaviour of D9 stainless steel – Zirconium metal waste form alloys
|
Bairi, Lipika Rani |
|
2010 |
52 |
7 |
p. 2291-2302 12 p. |
artikel |
22 |
Microstructure and corrosion of Pd-modified Ti alloys produced by powder metallurgy
|
Ashworth, M.A. |
|
2010 |
52 |
7 |
p. 2413-2421 9 p. |
artikel |
23 |
Nucleation and growth of selective oxide particles on ferritic steel
|
Ollivier-Leduc, A. |
|
2010 |
52 |
7 |
p. 2498-2504 7 p. |
artikel |
24 |
On the penetration of corrosion products from reinforcing steel into concrete due to chloride-induced corrosion
|
Wong, H.S. |
|
2010 |
52 |
7 |
p. 2469-2480 12 p. |
artikel |
25 |
Oxidation of stainless steel 304L in carbon dioxide
|
Goutier, F. |
|
2010 |
52 |
7 |
p. 2403-2412 10 p. |
artikel |
26 |
Role of water, acetic acid and chloride on corrosion and pitting behaviour of carbon steel in fuel-grade ethanol
|
Lou, Xiaoyuan |
|
2010 |
52 |
7 |
p. 2303-2315 13 p. |
artikel |
27 |
Single particle impingement current transients for prediction of erosion-enhanced corrosion on 304 stainless steel
|
Mohammadi, Farzad |
|
2010 |
52 |
7 |
p. 2331-2340 10 p. |
artikel |
28 |
Some particularities of the corrosion behaviour of Mg–Zn–Mn–Si–Ca alloys in alkaline chloride solutions
|
Lisitsyn, V. |
|
2010 |
52 |
7 |
p. 2280-2290 11 p. |
artikel |
29 |
Stability of MnCr2O4 spinel and Cr2O3 in high temperature carbonaceous environments with varied oxygen partial pressures
|
Li, Hao |
|
2010 |
52 |
7 |
p. 2481-2488 8 p. |
artikel |
30 |
Synergistic effect of iodide ion and polyacrylic acid on corrosion inhibition of iron in H2SO4 investigated by electrochemical techniques
|
Umoren, S.A. |
|
2010 |
52 |
7 |
p. 2422-2429 8 p. |
artikel |
31 |
The anodic dissolution of Mg in NaCl and Na2SO4 electrolytes by atomic emission spectroelectrochemistry
|
Światowska, Jolanta |
|
2010 |
52 |
7 |
p. 2372-2378 7 p. |
artikel |
32 |
The behaviour of second phase particles during anodizing of aluminium alloys
|
Saenz de Miera, M. |
|
2010 |
52 |
7 |
p. 2489-2497 9 p. |
artikel |
33 |
The negative difference effect of magnesium and of the AZ91 alloy in chloride and stannate-containing solutions
|
Thomaz, T.R. |
|
2010 |
52 |
7 |
p. 2235-2243 9 p. |
artikel |
34 |
The role of structural chemistry in the inhibitive performance of some aminopyrimidines on the corrosion of steel
|
Masoud, M.S. |
|
2010 |
52 |
7 |
p. 2387-2396 10 p. |
artikel |
35 |
XPS analysis of manganese in stainless steel passive films on 1.4432 and the lean duplex 1.4162
|
Fredriksson, W. |
|
2010 |
52 |
7 |
p. 2505-2510 6 p. |
artikel |