nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Abrasion-corrosion studies of passive stainless steels in acidic media using acoustic emission techniques
|
Oltra, R. |
|
1993 |
35 |
1-4 |
p. 641-645 5 p. |
artikel |
2 |
A corrosion fatigue study of zirconium in hot nitric acid
|
Popp, W. |
|
1993 |
35 |
1-4 |
p. 621-625 5 p. |
artikel |
3 |
Advances in understanding hydrodynamic effects on corrosion
|
Poulson, Bryan |
|
1993 |
35 |
1-4 |
p. 655-661 7 p. |
artikel |
4 |
An improvement of the resistance to stress-corrosion cracking of drawn copper wire
|
Ohnishi, H. |
|
1993 |
35 |
1-4 |
p. 471-473 3 p. |
artikel |
5 |
Anodic dissolution and passivation of Ni IN acid organic aprotic solvents
|
Ercolano, L. |
|
1993 |
35 |
1-4 |
p. 161-167 7 p. |
artikel |
6 |
A novel electrode assembly for studying corrosion of stainless steels by sulphate-reducing bacteria
|
Webster, B.J. |
|
1993 |
35 |
1-4 |
p. 675-679 5 p. |
artikel |
7 |
A photoelectrochemical study on anodic tantalum oxide films
|
Di Quarto, F. |
|
1993 |
35 |
1-4 |
p. 801-808 8 p. |
artikel |
8 |
Applications of deterministic chaos theory to corrosion
|
Stringer, J. |
|
1993 |
35 |
1-4 |
p. 751-760 10 p. |
artikel |
9 |
Applications of the scanning reference electrode technique to localized corrosion
|
Trethewey, K.R. |
|
1993 |
35 |
1-4 |
p. 127-129 3 p. |
artikel |
10 |
Aspects of galvanic corrosion behaviour of a range of materials in seawater
|
Hodgkiess, T. |
|
1993 |
35 |
1-4 |
p. 269-275 7 p. |
artikel |
11 |
Assessment of specific environments by metal piece test kits
|
Iikawa, Tsutomu |
|
1993 |
35 |
1-4 |
p. 735-742 8 p. |
artikel |
12 |
A study of the mechanism of A.C. electrolytic graining of aluminium in hydrochloric and nitric acid
|
Laevers, P. |
|
1993 |
35 |
1-4 |
p. 231-235 5 p. |
artikel |
13 |
A transmission electron microscopy study of stress corrosion cracking in stainless steels
|
Nisbet, W.J. |
|
1993 |
35 |
1-4 |
p. 457-469 13 p. |
artikel |
14 |
Characterization of the crevice solution chemistry of 304 stainless steel
|
Nash, B.K. |
|
1993 |
35 |
1-4 |
p. 817-825 9 p. |
artikel |
15 |
Chemical and electrochemical conditions within corrosion fatigue cracks
|
En-Hou, Han |
|
1993 |
35 |
1-4 |
p. 599-610 12 p. |
artikel |
16 |
Conference introductory paper why Manchester?
|
Wood, G.C. |
|
1993 |
35 |
1-4 |
p. 1-12 12 p. |
artikel |
17 |
Corrosion behavior of carbon fiber composites in the marine environment
|
Alias, M.N. |
|
1993 |
35 |
1-4 |
p. 395-402 8 p. |
artikel |
18 |
Corrosion behaviour of low-manganese stainless steels
|
Szummer, A. |
|
1993 |
35 |
1-4 |
p. 317-327 11 p. |
artikel |
19 |
Corrosion fatigue resistances of surgical implant stainless steels and titanium alloy
|
Yu, J. |
|
1993 |
35 |
1-4 |
p. 587-591 5 p. |
artikel |
20 |
Corrosion mechanism of tin-zinc alloys in neutral medium
|
Szira´ki, L. |
|
1993 |
35 |
1-4 |
p. 371-376 6 p. |
artikel |
21 |
Corrosion of protected aluminum and zinc
|
Hazan, Joseph |
|
1993 |
35 |
1-4 |
p. 223-229 7 p. |
artikel |
22 |
Corrosion resistance of different materials in dilute ammonium chloride-bearing environments
|
Forse´n, O. |
|
1993 |
35 |
1-4 |
p. 297-301 5 p. |
artikel |
23 |
Corrosion-resistant amorphous surface alloys
|
Hashimoto, K. |
|
1993 |
35 |
1-4 |
p. 363-370 8 p. |
artikel |
24 |
Crack initiation in the corrosion fatigue of structural steels in salt solutions
|
Boukerrou, A. |
|
1993 |
35 |
1-4 |
p. 577-585 9 p. |
artikel |
25 |
Design of ion-implanted coatings to impede hydrogen contamination of steel
|
Fassini, F.D. |
|
1993 |
35 |
1-4 |
p. 549-556 8 p. |
artikel |
26 |
Editorial
|
Scully, John |
|
1993 |
35 |
1-4 |
p. iii- 1 p. |
artikel |
27 |
Editorial Board
|
|
|
1993 |
35 |
1-4 |
p. CO2- 1 p. |
artikel |
28 |
Effect of atmospheric corrosion on the mechanical properties of the weathering steel ATMOFIX 52A
|
Kocich, Jaroslav |
|
1993 |
35 |
1-4 |
p. 719-725 7 p. |
artikel |
29 |
Effect of niobium doping on the atmospheric oxidation of Fe-Si-Al magnetic alloys
|
Konno, Hidetaka |
|
1993 |
35 |
1-4 |
p. 727-734 8 p. |
artikel |
30 |
Effects of dry deposition of pollutant gases on the degradation of pentelic marble
|
Haneef, S.J. |
|
1993 |
35 |
1-4 |
p. 743-747 5 p. |
artikel |
31 |
Effects of nickel and chromium on corrosion rate of linepipe steel
|
Denpo, K. |
|
1993 |
35 |
1-4 |
p. 285-288 4 p. |
artikel |
32 |
Electrochemical and corrosion behaviour of iridium-palladium oxide electrode prepared by electrochemical methods
|
Lee, Yuan-Po |
|
1993 |
35 |
1-4 |
p. 387-389 3 p. |
artikel |
33 |
Electrochemical assessment and monitoring of stabilisation of heavily corroded archaeological iron artefacts
|
Hjelm-Hansen, N. |
|
1993 |
35 |
1-4 |
p. 767-774 8 p. |
artikel |
34 |
Electrochemical characteristics of the Al2Cu, Al3Ta and Al3Zr intermetallic phases and their relevancy to the localized corrosion of Al alloys
|
Scully, J.R. |
|
1993 |
35 |
1-4 |
p. 185-195 11 p. |
artikel |
35 |
Electrochemical characterization of the corrosion resistance of aluminum-lithium alloys
|
Roberge, P.R. |
|
1993 |
35 |
1-4 |
p. 213-221 9 p. |
artikel |
36 |
Electrochemical experiments on UO2 corrosion in aqueous solutions
|
Bottomley, P.D.W. |
|
1993 |
35 |
1-4 |
p. 377-383 7 p. |
artikel |
37 |
Environmental cracking of AISI 4145 steel in drilling muds
|
Gonzalez-Rodriguez, J.G. |
|
1993 |
35 |
1-4 |
p. 515-520 6 p. |
artikel |
38 |
Environmental effects on crack closure in the corrosion fatigue of an aluminium-lithium alloy
|
Pyun, Su-Il |
|
1993 |
35 |
1-4 |
p. 611-617 7 p. |
artikel |
39 |
Erosion-corrosion of passive metals by solid particles
|
Nova´k, P. |
|
1993 |
35 |
1-4 |
p. 635-640 6 p. |
artikel |
40 |
Exceedances, extremes, extrapolation and order statistics for pits, pitting and other localized corrosion phenomena
|
Laycock, P.J. |
|
1993 |
35 |
1-4 |
p. 135-145 11 p. |
artikel |
41 |
Factors influencing stress corrosion cracking of high strength pearlitic steels
|
Toribio, J. |
|
1993 |
35 |
1-4 |
p. 521-530 10 p. |
artikel |
42 |
Fracture morphologies exhibited by commercially pure titanium when strained to failure while in contact with chloride-containing environments
|
Simbi, D.J. |
|
1993 |
35 |
1-4 |
p. 489-497 9 p. |
artikel |
43 |
Hydrogen embrittlement susceptibility of galvanized 4135 steel in cement environment
|
Roberge, Re´al |
|
1993 |
35 |
1-4 |
p. 507-514 8 p. |
artikel |
44 |
Hydrogen trapping at phosphorus-segregated grain boundaries in nickel-chromium steel
|
Pyun, Su-Il |
|
1993 |
35 |
1-4 |
p. 531-533 3 p. |
artikel |
45 |
In situ studies of passive film chemistry using X-ray absorption spectroscopy
|
Davenport, Alison J. |
|
1993 |
35 |
1-4 |
p. 19-25 7 p. |
artikel |
46 |
In situ synchrotron radiation X-ray techniques for studies of corrosion and protection
|
Robinson, J. |
|
1993 |
35 |
1-4 |
p. 791-800 10 p. |
artikel |
47 |
Intuition, case work and testing: A holistic approach to the corrosion of a 12% chromium steel in aqueous environments
|
McEwan, J.J. |
|
1993 |
35 |
1-4 |
p. 303-315 13 p. |
artikel |
48 |
Ion beam surface modification of aluminum
|
McCafferty, E. |
|
1993 |
35 |
1-4 |
p. 239-246 8 p. |
artikel |
49 |
Laser depassivation of a channel flow double-electrode: A new technique in repassivation studies
|
Oltra, R. |
|
1993 |
35 |
1-4 |
p. 827-832 6 p. |
artikel |
50 |
Local corrosion processes in the presence of sulphate-reducing bacteria: Measurements under biofilms
|
Pourbaix, Antoine |
|
1993 |
35 |
1-4 |
p. 693-698 6 p. |
artikel |
51 |
Mechanisms of underdeposit corrosion in freshwater cooled austenitic alloy heat exchangers
|
Brennenstuhl, A.M. |
|
1993 |
35 |
1-4 |
p. 699-705 7 p. |
artikel |
52 |
Microscopic and local probe method for studying crevice corrosion and its application to iron and stainless steel
|
Pickering, Howard W. |
|
1993 |
35 |
1-4 |
p. 775-781 7 p. |
artikel |
53 |
Modelling the stress corrosion cracking of low alloy steels
|
Gutierrez-Solana, F. |
|
1993 |
35 |
1-4 |
p. 499-505 7 p. |
artikel |
54 |
Moire method to measure penetration depth profiles on unevenly corroded metal surfaces
|
Shinohara, Tadashi |
|
1993 |
35 |
1-4 |
p. 785-789 5 p. |
artikel |
55 |
Nickel release from 304 and 316 stainless steels in synthetic sweat. Comparison with nickel and nickel-plated metals. Consequences on allergic contact dermatitis
|
Haudrechy, P. |
|
1993 |
35 |
1-4 |
p. 329-336 8 p. |
artikel |
56 |
Non-destructive testing using electromagnetic impedance spectroscopy
|
Williams, L.A. |
|
1993 |
35 |
1-4 |
p. 833-839 7 p. |
artikel |
57 |
On the corrosion characterization of titanium nitride in sulfuric acid solution
|
Chyou, S.D. |
|
1993 |
35 |
1-4 |
p. 337-341 5 p. |
artikel |
58 |
On the passivation characteristics of a β-FeAl intermetallic compound in sulphate solutions
|
Frangini, S. |
|
1993 |
35 |
1-4 |
p. 153-159 7 p. |
artikel |
59 |
Passivation thresholds in iron-chromium alloys prepared by ion-beam sputtering
|
Fujimoto, S. |
|
1993 |
35 |
1-4 |
p. 51-55 5 p. |
artikel |
60 |
Passive films on stainless steels after gamma-ray irradiation, as studied by electrochemical impedance spectroscopy
|
Capobianco, G. |
|
1993 |
35 |
1-4 |
p. 35-41 7 p. |
artikel |
61 |
Performance of high-alloy austenitic stainless steels in the actual and simulated bleaching media of the paper industry
|
Stampella, R.S. |
|
1993 |
35 |
1-4 |
p. 289-295 7 p. |
artikel |
62 |
Pitting corrosion of electroplated permalloy films
|
Frankel, G.S. |
|
1993 |
35 |
1-4 |
p. 63-71 9 p. |
artikel |
63 |
Potential transmission and transients during corrosion: Applications to corrosion monitoring
|
Isaacs, Hugh S. |
|
1993 |
35 |
1-4 |
p. 97-101 5 p. |
artikel |
64 |
Predictive models for erosion-corrosion under disturbed flow conditions
|
Postlethwaite, J. |
|
1993 |
35 |
1-4 |
p. 627-633 7 p. |
artikel |
65 |
Preface
|
Procter, R.P.M. |
|
1993 |
35 |
1-4 |
p. v-vi nvt p. |
artikel |
66 |
Quantitative measurements of the degree of exfoliation on aluminium alloys
|
Habashi, M. |
|
1993 |
35 |
1-4 |
p. 169-183 15 p. |
artikel |
67 |
Salt film development during pitting of nickel
|
Luo, J.L. |
|
1993 |
35 |
1-4 |
p. 73-81 9 p. |
artikel |
68 |
Stability of minority phases in some corrosion media
|
Bystriansky´, Jaroslav |
|
1993 |
35 |
1-4 |
p. 355-361 7 p. |
artikel |
69 |
Stress analysis aspects of the development of a standard test method for sour service testing
|
Fowler, C.M. |
|
1993 |
35 |
1-4 |
p. 541-548 8 p. |
artikel |
70 |
Stress corrosion cracking of carbon steel in caustic aluminate solutions of the Bayer process
|
Huy Ha Le, |
|
1993 |
35 |
1-4 |
p. 435-442 8 p. |
artikel |
71 |
Studies of passive films on amorphous Fe-Cr-(B,P,C) alloys
|
Virtanen, S. |
|
1993 |
35 |
1-4 |
p. 27-34 8 p. |
artikel |
72 |
Studies of the inhibiting effect of 1,2,3-benzotriazole on the stress-corrosion cracking of 70/30 brass in fluoride environments
|
Shih, H.C. |
|
1993 |
35 |
1-4 |
p. 479-483 5 p. |
artikel |
73 |
Surface hydrogen profiling in metallic materials by the elastic recoil detection technique
|
Bott, A.H. |
|
1993 |
35 |
1-4 |
p. 557-563 7 p. |
artikel |
74 |
Surface mobility mechanism of stress-corrosion cracking
|
Galvele, J.R. |
|
1993 |
35 |
1-4 |
p. 419-434 16 p. |
artikel |
75 |
Synergism of alloying elements and pitting corrosion resistance of stainless steels
|
Lu, Y.C. |
|
1993 |
35 |
1-4 |
p. 89-96 8 p. |
artikel |
76 |
Testing the film-induced cleavage model of stress-corrosion cracking
|
Saito, M. |
|
1993 |
35 |
1-4 |
p. 411-413 3 p. |
artikel |
77 |
The achilles expert system on corrosion and protection: Consultations on aspects of stress corrosion cracking
|
Smart, N.R. |
|
1993 |
35 |
1-4 |
p. 403-410 8 p. |
artikel |
78 |
The activation of aluminium by activator elements
|
Breslin, C.B. |
|
1993 |
35 |
1-4 |
p. 197-203 7 p. |
artikel |
79 |
The behaviour of corrosion-resistant steels in seawater: A review
|
Bardal, Einar |
|
1993 |
35 |
1-4 |
p. 257-267 11 p. |
artikel |
80 |
The blistering phenomenon in zirconium and zirconium alloys
|
Golozar, M.A. |
|
1993 |
35 |
1-4 |
p. 565-567 3 p. |
artikel |
81 |
The chemical state of copper in high-Tc cuprate superconductors and the consequential corrosion of electrical contacts
|
Goddard, D.T. |
|
1993 |
35 |
1-4 |
p. 761-766 6 p. |
artikel |
82 |
The corrosion of aluminium in halogenated hydrocarbon solvents
|
Bretherton, N. |
|
1993 |
35 |
1-4 |
p. 205-211 7 p. |
artikel |
83 |
The corrosion of Ni-Cr dental alloys studied byin situ raman spectroscopy: Role of beryllium
|
Bernard, M.C. |
|
1993 |
35 |
1-4 |
p. 809-815 7 p. |
artikel |
84 |
The development of chemical conversion coatings on aluminium
|
Brown, G.M. |
|
1993 |
35 |
1-4 |
p. 253-256 4 p. |
artikel |
85 |
The dissolution and repassivation kinetics of Fe-Cr alloys in pit solutions
|
Steinsmo, Unni |
|
1993 |
35 |
1-4 |
p. 83-88 6 p. |
artikel |
86 |
The effect of sulphate-reducing bacteria on the electrochemical behaviour of corrosion-resistant alloys in sea water
|
Gouda, V.K. |
|
1993 |
35 |
1-4 |
p. 683-689 7 p. |
artikel |
87 |
The effects of dilution upon the corrosion and wear properties of cobalt-based weld overlays
|
Crook, P. |
|
1993 |
35 |
1-4 |
p. 647-653 7 p. |
artikel |
88 |
The electrochemical conditions for coloured film formation on type 304 stainless steel with square wave polarization
|
Fujimoto, Shinji |
|
1993 |
35 |
1-4 |
p. 147-152 6 p. |
artikel |
89 |
The electrochemistry of iron, zinc and copper in thin layer electrolytes
|
Zhang, S.H. |
|
1993 |
35 |
1-4 |
p. 713-718 6 p. |
artikel |
90 |
The growth and stability of passive films
|
Graham, M.J. |
|
1993 |
35 |
1-4 |
p. 13-18 6 p. |
artikel |
91 |
The influence of pulverised fuel ash on the corrosion rate of titanium
|
Eley, C.D. |
|
1993 |
35 |
1-4 |
p. 349-354 6 p. |
artikel |
92 |
The nucleation and growth of corrosion pits on stainless steel
|
Burstein, G.T. |
|
1993 |
35 |
1-4 |
p. 57-62 6 p. |
artikel |
93 |
The pitting corrosion of plasma nitrided chromium steels in sulphate solution
|
Mankowski, J. |
|
1993 |
35 |
1-4 |
p. 111-116 6 p. |
artikel |
94 |
The pitting corrosion of p-type GaAs single crystals
|
Tromans, Desmond |
|
1993 |
35 |
1-4 |
p. 117-125 9 p. |
artikel |
95 |
The pitting of low alloy turbine disc steel
|
Otieno-Alego, V. |
|
1993 |
35 |
1-4 |
p. 103-109 7 p. |
artikel |
96 |
The stress corrosion cracking of austenitic stainless steels in H3BO3 + NaCl solutions between 100°C and 200°C
|
Kasri, R. |
|
1993 |
35 |
1-4 |
p. 443-451 9 p. |
artikel |
97 |
The stress-corrosion cracking of iron-boron-silicon metallic glasses
|
Habib, K. |
|
1993 |
35 |
1-4 |
p. 571-573 3 p. |
artikel |
98 |
The surface characterization of titanium and titanium-nickel alloys in sulfuric acid
|
Asami, K. |
|
1993 |
35 |
1-4 |
p. 43-49 7 p. |
artikel |
99 |
Thin surface films on metals and alloys
|
Shimizu, K. |
|
1993 |
35 |
1-4 |
p. 247-252 6 p. |
artikel |
100 |
What progress in the understanding of microbially induced corrosion has been made in the last 25 years? A personal viewpoint
|
Stott, J.F.D. |
|
1993 |
35 |
1-4 |
p. 667-673 7 p. |
artikel |