nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
Aluminizing of iron-nickel-base alloys for resistance to high-temperature gaseous environments
|
Green, S.W. |
|
1992 |
33 |
3 |
p. 345-359 15 p. |
artikel |
2 |
An electrochemical and surface analytical study of stainless steels and titanium exposed to natural seawater
|
Mansfeld, Florian |
|
1992 |
33 |
3 |
p. 445-456 12 p. |
artikel |
3 |
Announcement
|
|
|
1992 |
33 |
3 |
p. 509- 1 p. |
artikel |
4 |
A persistent corrosion-protective film formed on iron in acid solutions with triethylbismuthine
|
Ihara, Masaru |
|
1992 |
33 |
3 |
p. 389-397 9 p. |
artikel |
5 |
Corrosion diary
|
|
|
1992 |
33 |
3 |
p. 511-512 2 p. |
artikel |
6 |
Electrochemical and XPS studies on lacquer—low tinplated steel adhesion
|
Ingo, G.M. |
|
1992 |
33 |
3 |
p. 361-377 17 p. |
artikel |
7 |
Evolution of the corrosion potential of repassivating aluminium surfaces
|
Burstein, G.T |
|
1992 |
33 |
3 |
p. 475-492 18 p. |
artikel |
8 |
On the linear response of a passivated metallic electrode to potential step perturbation
|
Song, Guangling |
|
1992 |
33 |
3 |
p. 413-423 11 p. |
artikel |
9 |
Potentiostatic testing of plasma-deposited silicon nitride thin protective films for bonds, bondwires and bondpads in microelectronic assemblies
|
Ulrich, Richard K. |
|
1992 |
33 |
3 |
p. 403-412 10 p. |
artikel |
10 |
The corrosion behavior of sputter-deposited AlZr alloys in 1 M HCl solution
|
Yoshioka, H. |
|
1992 |
33 |
3 |
p. 425-436 12 p. |
artikel |
11 |
The duplex structure of cell walls of porous anodic films formed on aluminum
|
Ono, Sachiko |
|
1992 |
33 |
3 |
p. 503-505 3 p. |
artikel |
12 |
The effect of amino acids on the corrosion of nickel in H2SO4
|
Aksüt, A.A. |
|
1992 |
33 |
3 |
p. 379-387 9 p. |
artikel |
13 |
The effects of chromate on the transient repassivation potential of aluminium in chloride solution
|
Cinderey, R.J. |
|
1992 |
33 |
3 |
p. 493-498 6 p. |
artikel |
14 |
The initiation of pitting corrosion on austenitic stainless steel: on the role and importance of sulphide inclusions
|
Stewart, J. |
|
1992 |
33 |
3 |
p. 457-463 7 p. |
artikel |
15 |
The passivation of aluminium in lithium carbonate/bicarbonate solutions
|
Rangel, C.M. |
|
1992 |
33 |
3 |
p. 327-343 17 p. |
artikel |
16 |
The repassivation potential of aluminium in water
|
Cinderey, R.J. |
|
1992 |
33 |
3 |
p. 499-502 4 p. |
artikel |
17 |
The role of hydrogen in the pitting of passivating films on pure iron
|
Pyun, Su-Il |
|
1992 |
33 |
3 |
p. 437-444 8 p. |
artikel |