nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
An X-ray photo-emission spectroscopy study of iron-oxide, iron-benzoic acid inhibitor films
|
Wood, J.C. |
|
1978 |
18 |
4 |
p. 315-321 7 p. |
artikel |
2 |
[No title]
|
Johnson, J.B. |
|
1978 |
18 |
4 |
p. 407-408 2 p. |
artikel |
3 |
Stress corrosion cracking of a high strength steel in saturated Ca(OH)2 solutions caused by CL and SO2 4 additions
|
Eickemeyer, Jörg |
|
1978 |
18 |
4 |
p. 397-400 4 p. |
artikel |
4 |
Sulphidation of copper-nickel alloys—II. Scale growth kinetics
|
Bastow, B.D. |
|
1978 |
18 |
4 |
p. 297-313 17 p. |
artikel |
5 |
Sulphidation of copper-nickel alloys—I. Scale morphologies
|
Bastow, B.D. |
|
1978 |
18 |
4 |
p. 275-295 21 p. |
artikel |
6 |
The dissolution of magnetite in acidic perchlorate solutions
|
Haruyama, Shiro |
|
1978 |
18 |
4 |
p. 263-274 12 p. |
artikel |
7 |
The effect of pH, copper content and ammonia concentration on the stress corrosion cracking susceptibility of an aged Cu−4%Ti alloy
|
Takemoto, T. |
|
1978 |
18 |
4 |
p. 323-336 14 p. |
artikel |
8 |
The identification, formation and influence of a strongly epitaxial oxide phase during selective oxidation of an Fe-Cr alloy
|
Crouch, I.G. |
|
1978 |
18 |
4 |
p. 401-405 5 p. |
artikel |
9 |
The protection of 9% chromium steels using vapour-deposited silica coatings
|
Brown, A.M. |
|
1978 |
18 |
4 |
p. 337-349 13 p. |
artikel |
10 |
The sensitization of ferritic steels containing less than 12% Cr
|
Poulson, Bryan |
|
1978 |
18 |
4 |
p. 371-395 25 p. |
artikel |
11 |
The treatment of rusted steel with mimosa tannin
|
Ross, T.K. |
|
1978 |
18 |
4 |
p. 351-361 11 p. |
artikel |
12 |
The use of soluble corrosion inhibitors for aluminium alloys
|
Salem, T.M. |
|
1978 |
18 |
4 |
p. 363-369 7 p. |
artikel |