nr |
titel |
auteur |
tijdschrift |
jaar |
jaarg. |
afl. |
pagina('s) |
type |
1 |
An AZ31 magnesium alloy coating for protecting polyimide from erosion-corrosion by atomic oxygen
|
Qi, Hong |
|
|
138 |
C |
p. 170-177 |
artikel |
2 |
An electrochemical study on the effect of stabilization and sensitization heat treatments on the intergranular corrosion behaviour of AISI 321H austenitic stainless steel
|
Morshed-Behbahani, Khashayar |
|
|
138 |
C |
p. 28-41 |
artikel |
3 |
Comparison of the oxidation behavior of a zirconium nitride coating in water vapor and air at high temperature
|
Gao, Zhaohe |
|
|
138 |
C |
p. 242-251 |
artikel |
4 |
Corrigendum to “Spreading of intergranular corrosion on the surface of sensitized Al-4.4 Mg alloys: A general finding” [Corros. Sci. 59 (2012) 136–147]
|
Jain, Swati |
|
|
138 |
C |
p. 178 |
artikel |
5 |
Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water
|
Guo, Xianglong |
|
|
138 |
C |
p. 297-306 |
artikel |
6 |
Corrosion resistant nickel coating with strong adhesion on AZ31B magnesium alloy prepared by an in-situ shot-peening-assisted cold spray
|
Wei, Ying-Kang |
|
|
138 |
C |
p. 105-115 |
artikel |
7 |
Degradation of concrete with addition of mineral admixture due to free chloride ion penetration under the effect of carbonation
|
Jin, Ming |
|
|
138 |
C |
p. 42-53 |
artikel |
8 |
Development of gradient microstructure in mild steel and grain size dependence of its electrochemical response
|
Rai, Prabhat K. |
|
|
138 |
C |
p. 85-95 |
artikel |
9 |
3D time-resolved observations of corrosion and corrosion-fatigue crack initiation and growth in peak-aged Al 7075 using synchrotron X-ray tomography
|
Stannard, Tyler J. |
|
|
138 |
C |
p. 340-352 |
artikel |
10 |
Editorial Board
|
|
|
|
138 |
C |
p. ii |
artikel |
11 |
Effect of doping anions on the degradation of electrochemical activity of conductive polypyrrole in NaOH solution
|
Jin, Zhenzhen |
|
|
138 |
C |
p. 252-265 |
artikel |
12 |
Effect of pre-oxidation on the oxidation resistance of Crofer 22 APU
|
Talic, Belma |
|
|
138 |
C |
p. 189-199 |
artikel |
13 |
Effect of surface abrasion on pitting corrosion of Al-Li alloy
|
Liu, Jianhua |
|
|
138 |
C |
p. 75-84 |
artikel |
14 |
Effect of sustained load and seawater and sea sand concrete environment on durability of basalt- and glass-fibre reinforced polymer (B/GFRP) bars
|
Wang, Zike |
|
|
138 |
C |
p. 200-218 |
artikel |
15 |
Effects of Cr addition on thermal stability, soft magnetic properties and corrosion resistance of FeSiB amorphous alloys
|
Xu, D.D. |
|
|
138 |
C |
p. 20-27 |
artikel |
16 |
Electrochemical response of micro-alloyed steel under potentiostatic polarization in CO2 saturated brine
|
Onyeji, Lawrence |
|
|
138 |
C |
p. 146-153 |
artikel |
17 |
Enhanced corrosion protection of mild steel by the synergetic effect of zinc aluminum polyphosphate and 2-mercaptobenzimidazole inhibitors incorporated in epoxy-polyamide coatings
|
Mirzakhanzadeh, Z. |
|
|
138 |
C |
p. 372-379 |
artikel |
18 |
Enhanced corrosion resistance of AZ91 magnesium alloy through refinement and homogenization of surface microstructure by friction stir processing
|
Liu, Qu |
|
|
138 |
C |
p. 284-296 |
artikel |
19 |
Excellent superhydrophobic surface and anti-corrosion performance by nanostructure of discotic columnar liquid crystals
|
Liu, Yu-Chiao |
|
|
138 |
C |
p. 1-7 |
artikel |
20 |
Fabrication of the lamellar NiAl nanochannel by selective phase dissolution of NiAl–Cr(Mo) eutectic alloy
|
Wei, Lufeng |
|
|
138 |
C |
p. 142-145 |
artikel |
21 |
Flow cell apparatus for quantitative evaluation of carbon steel corrosion during transitions in fluid composition: Application to transition from inhibited hydrochloric acid to sodium chloride brine
|
Barker, Richard |
|
|
138 |
C |
p. 116-129 |
artikel |
22 |
Inhibitory effect of three phenacyl derivatives on the oxidation of sphalerite (ZnS) in air-equilibrated acidic solution
|
Chiriţă, Paul |
|
|
138 |
C |
p. 154-162 |
artikel |
23 |
Isothermal oxidation of the Ti2AlC MAX phase coatings deposited by kerosene-fuelled HVOF spray
|
Zhang, Zheng |
|
|
138 |
C |
p. 266-274 |
artikel |
24 |
Kinetic study and modelling of silver dissolution in synthetic industrial silver electrolyte as a function of electrolyte composition and temperature
|
Aji, Arif T. |
|
|
138 |
C |
p. 163-169 |
artikel |
25 |
New insight into δ-Pu alloy oxidation kinetics highlighted by using in-situ X-ray diffraction coupled with an original Rietveld refinement method
|
Ravat, B. |
|
|
138 |
C |
p. 66-74 |
artikel |
26 |
Photo and thermally stable branched corrosion inhibitors containing two benzotriazole groups for copper in 3.5 wt% sodium chloride solution
|
Jing, Chuan |
|
|
138 |
C |
p. 353-371 |
artikel |
27 |
Rapid colorimetric analysis of graphene on copper
|
Candadai, Aaditya A. |
|
|
138 |
C |
p. 319-325 |
artikel |
28 |
Role of Al2O3 inclusions on the localized corrosion of Q460NH weathering steel in marine environment
|
Liu, Chao |
|
|
138 |
C |
p. 96-104 |
artikel |
29 |
Sensitization and remediation effects on environmentally assisted cracking of Al-Mg naval alloys
|
Seifi, M. |
|
|
138 |
C |
p. 219-241 |
artikel |
30 |
Severe corrosion of steel and copper by strontium bromide in thermochemical heat storage reactors
|
D’Ans, Pierre |
|
|
138 |
C |
p. 275-283 |
artikel |
31 |
Sol–gel grown MgO-ZnO-tricalcium-phosphate nanobioceramics: Evaluation of mechanical and degradation attributes
|
Said Mahraz, Zahra Ashur |
|
|
138 |
C |
p. 179-188 |
artikel |
32 |
Steam oxidation resistance and performance of newly developed coatings for Haynes® 282® Ni-based alloy
|
Dudziak, T. |
|
|
138 |
C |
p. 326-339 |
artikel |
33 |
Stress corrosion crack initiation in machined type 316L austenitic stainless steel in simulated pressurized water reactor primary water
|
Chang, Litao |
|
|
138 |
C |
p. 54-65 |
artikel |
34 |
Study of simulated disbonded polymer film on Zn-Al alloy coated reinforcing steel rebars
|
Abdulsalam, Mohammed I. |
|
|
138 |
C |
p. 307-318 |
artikel |
35 |
The corrosion behavior of Ni-Cu gradient layer on the nickel aluminum-bronze (NAB) alloy
|
Luo, Qin |
|
|
138 |
C |
p. 8-19 |
artikel |
36 |
The study on the corrosion mechanism of protective ternary ZnFeMo alloy coatings deposited on carbon steel in 0.5 mol dm–3 NaCl solution
|
Winiarski, J. |
|
|
138 |
C |
p. 130-141 |
artikel |